Borosilicate glasses with low alkali content
Abstract
According to one embodiment, a glass may include from about 50 mol. % to about 70 mol. % SiO2; from about 12 mol. % to about 35 mol. % B2O3; from about 4 mol. % to about 12 mol. % Al2O3; greater than 0 mol. % and less than or equal to 1 mol. % alkali metal oxide, wherein Li2O is greater than or equal to about 20% of the alkali metal oxide; from about 0.3 mol. % to about 0.7 mol. % of Na2O or Li2O; and greater than 0 mol. % and less than 12 mol. % of total divalent oxide, wherein the total divalent oxide includes at least one of CaO, MgO and SrO, and wherein a ratio of Li2O (mol. %) to (Li2O (mol. %)+(Na2O (mol. %)) is greater than or equal 0.4 and less than or equal to 0.6. The glass may have a relatively low high temperature resistivity and a relatively high low temperature resistivity.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 35 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A glass article comprising: a core glass; a clad glass fused to the core glass, wherein: the clad glass comprises from 50 mol. % to 70 mol. % SiO 2 ; the clad glass comprises from 12 mol. % to 35 mol. % B 2 O 3 ; the clad glass comprises from 4 mol. % to 12 mol. % Al 2 O 3 ; the clad glass comprises alkali metal oxide, the alkali metal oxide comprising at least one of Na 2 O, Li 2 O, and K 2 O, wherein Na 2 O and/or Li 2 O is from 0.3 mol. % to 0.6 mol. % in the clad glass, Li 2 O is greater than or equal to 20% of the alkali metal oxide in the clad glass, the ratio of Li 2 O (mol. %) to (Li 2
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (35)
Non-Patent Literature (5)
- ASTM 0598-93(2013), titled “Standard Test for Annealing Point and Strain Point of Glass by Beam Bending.”
- ASTM 0657-93(2013), titled “Standard Test Method for D-C Volume Resistivity of Glass.”
- ASTM 0965-96(2012), titled “Standard Practice for Measuring Viscosity of Glass Above the Softening Point.”.
- ASTM C829-81 (2015), titled “Standard Practice for Measurement of L˜iquidus Temperature of Glass by the Gradient Furnace Method.”
- Astm D257.3859 (2016), titled “Standard Test Methods for DC Resistance or Conductance of Insulating Materials.”