Patents
US 11,569,441 B2#118733802 Most CitedActiveUnited States (USPTO)Utility

Maintaining coercive field after high temperature anneal for magnetic device applications with perpendicular magnetic anistropy

0Forward Citations (#118733802 Global)
0.0/yrCitation Velocity (#118733802 Global)
0.56Citation PageRank (#118733802 Global)
24Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A magnetic tunnel junction with perpendicular magnetic anisotropy (PMA MTJ) is disclosed wherein a free layer interfaces with a tunnel barrier and has a second interface with an oxide layer. A lattice-matching layer adjoins an opposite side of the oxide layer with respect to the free layer and is comprised of CoXFeYNiZLWMV or an oxide or nitride of Ru, Ta, Ti, or Si, wherein L is one of B, Zr, Nb, Hf, Mo, Cu, Cr, Mg, Ta, Ti, Au, Ag, or P, and M is one of Mo, Mg, Ta, Cr, W, or V, (x+y+z+w+v)=100 atomic %, x+y>0, and each of v and w are >0. The lattice-matching layer grows a BCC structure during annealing thereby promoting BCC structure growth in the oxide layer that results in enhanced free layer PMA and improved thermal stability.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method comprising: providing a stack of layers that includes a reference layer, a tunnel barrier, and a free layer; forming an oxide layer on the free layer; forming a lattice-matching layer on the oxide layer; forming a hard mask on the first lattice-matching layer; and annealing the lattice-matching layer so that the lattice-matching layer grows a body centered cubic (BCC) structure.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the lattice-matching layer includes non-magnetic metals or alloys.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the lattice-matching layer includes non-magnetic metals or alloys of M, and wherein M is selected from the group consisting of Mo, Mg, Ta, Cr, W, Ru and V.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (24)

PatentTitleYearCitations
US 6,544,801 B1Method of fabricating thermally stable MTJ cell and apparatus200396
US 2007253122 A1Magneto-resistive element and method of manufacturing the same—53
US 2010034014 A1Magnetoresistive Element, Magnetic Memory Cell and Magnetic Random Access Memory Using the Same—22
US 2010148167 A1Magnetic tunnel junction stack—60
US 2012018825 A1Magnetic memory devices, electronic systems and memory cards including the same, methods of manufacturing the same, and methods of forming a perpendicular magnetic film of the same—25
US 2012155156 A1Method and system for providing magnetic tunneling junction elements having improved performance through capping layer induced perpendicular anisotropy and memories using such magnetic elements—50
US 2012205758 A1Magnetic element with improved out-of-plane anisotropy for spintronic applications—125
US 2012236631 A1Magnetic tunneling junction devices, memories, electronic systems, and memory systems, and methods of fabricating the same—26
US 2012280339 A1PERPENDICULAR MAGNETIC TUNNEL JUNCTION (pMTJ) WITH IN-PLANE MAGNETO-STATIC SWITCHING-ENHANCING LAYER—38
US 2012300542 A1Storage element and storage device—43
US 8,852,762 B2Magnetic random access memory with synthetic antiferromagnetic storage layers and non-pinned reference layers201410
US 2014349415 A1Perpendicular mtj stacks with magnetic anisotropy enhancing layer and crystallization barrier layer—7
US 8,912,614 B2Magnetic tunnel junction devices having magnetic layers formed on composite, obliquely deposited seed layers20144
US 2015008547 A1Hybridized Oxide Capping Layer for Perpendicular Magnetic Anisotropy—71
US 2015028439 A1Memory cells, methods of fabrication, semiconductor device structures, memory systems, and electronic systems—20
US 8,946,834 B2High thermal stability free layer with high out-of-plane anisotropy for magnetic device applications201540
US 9,006,704 B2Magnetic element with improved out-of-plane anisotropy for spintronic applications201544
US 9,130,155 B2Magnetic junctions having insertion layers and magnetic memories using the magnetic junctions201516
US 9,147,833 B2Hybridized oxide capping layer for perpendicular magnetic anisotropy201513
US 2015311252 A1Magnetic random access memory with ultrathin reference layer—13
US 9,425,387 B1Magnetic element with perpendicular magnetic anisotropy for high coercivity after high temperature annealing201648
WO 2016/178758 A1Magnetic tunnel junctions—9
US 9,966,529 B1MgO insertion into free layer for magnetic memory applications201811
US 2020028073 A1Maintaining Coercive Field after High Temperature Anneal for Magnetic Device Applications with Perpendicular Magnetic Anisotropy—1

Non-Patent Literature (5)

  • Garrels, Robert M., “Some Thermodynamic Relations Among the Vanadium Oxides and their Relation to the Oxidation State of the Uranium Ores of the Colorado Plateaus”, Aug. 1954, Am. Mineralogist, v. 38, pp. 1251-1265.
  • Ikeda, S., et al., “A perpendicular-anisotropy CoFeB-MgO magnetic tunneljunction”, Nature Materials, vol. 9, Sep. 2010, pp. 721-724, DOI: 10.1038/NMAT2804.
  • Kubota, Hitoshi, et al., “Enhancement of perpendicular magnetic anisotropy in Feb free layers using a thin MgO cap layer”, Journal of Applied Physics 111, 07C723, Mar. 2012.
  • PCT Search Report, International Application No. PCT/US2014/042251, Applicant: Headway Technologies, Inc., dated Oct. 13, 2014, 11 pgs.
  • PCT Search Report, International Application No. PCT/US2018/021007, Applicant: Headway Technologies, Inc., dated Jun. 22, 2018, 22 pages.