Abstract
A method for forming an oxide layer includes forming an interfacial layer on a substrate, forming an amorphous silicon layer on the interfacial layer, performing a direct oxidation process to selectively oxidize the formed amorphous silicon layer, and performing a thermal oxidation process to oxidize the formed amorphous silicon layer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for forming an oxide layer, comprising: forming an interfacial layer on a substrate; forming an amorphous silicon layer on the interfacial layer; performing a direct oxidation process to directly and selectively oxidize only a portion of the formed amorphous silicon layer; and performing a thermal oxidation process to oxidize a remaining non-oxidized portion of the formed amorphous silicon layer.
- Claim 2Depends on #1
The method of claim 1 , wherein the substrate comprises crystalline silicon, and the substrate includes concave shaped features and the oxide layer is formed within the concave shaped features.
- Claim 3Depends on #1
The method of claim 1 , wherein the interfacial layer comprises silicon oxide and has a thickness of between 2 Å and 20 Å.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (10)
Non-Patent Literature (1)
- International Search Report dated Jan. 3, 2022 for Application No. PCT/US2021/050601.