Patents
US 11,566,334 B2#132651856 Most CitedActiveUnited States (USPTO)Utility

Selective removal of noble metals using acidic fluids, including fluids containing nitrate ions

0Forward Citations (#132651856 Global)
0.0/yrCitation Velocity (#132651856 Global)
0.56Citation PageRank (#132651856 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The recovery of noble metal(s) from noble-metal-containing material is generally described. The noble metal(s) can be recovered selectively, in some cases, such that noble metal(s) is at least partially separated from non-noble-metal material within the material. Noble metal(s) may be recovered from noble-metal-containing material using mixtures of acids, in some instances. In some cases, the mixture can comprise nitric acid and/or another source of nitrate ions and at least one supplemental acid, such as sulfuric acid, phosphoric acid, and/or a sulfonic acid. The amount of nitrate ions within the mixture can be, in some instances, relatively small compared to the amount of supplemental acid within the mixture. In some cases, the recovery of noble metal(s) using the acid mixtures described herein can be enhanced by transporting an electric current between an electrode and the noble metal(s) of the noble-metal-containing material. In some cases, acid mixtures can be used to recover silver from particular types of scrap materials, such as scrap material comprising silver metal and cadmium oxide and/or scrap material comprising silver metal and tungsten metal.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method, comprising: exposing a material comprising at least one noble metal and at least one base metal to a mixture comprising nitrate ions and at least one sulfonic acid such that at least a portion of the at least one noble metal is removed from the material, wherein: the amount of nitrate ions within the mixture is less than or equal to about 10 wt %, and the total amount of the at least one sulfonic acid within the mixture is less than about 25 wt %.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the mixture further comprises sulfuric acid.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein the amount of sulfuric acid within the mixture is at least about 50 wt %.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 1,335,277 AProcess for the extraction and recovery of tungsten19206
US 2,185,858 AMethod of removing gold, silver, palladium, or the like194019
US 2,574,620 ABeta-di-piperonyl-amino-ethanol-hydrochloride19514
US 2,607,721 ASilver recovery from sodium thiosulfate solutions19525
US 2,794,829 APreparation of basic polyvalent metal salts of organic sulfonic acids195718
GB 934,850 AImprovements in processes and apparatuses for electrolytic treatments in the barrel—5
US 3,616,332 AProcess for recovering silver from scrap materials and electrolyte composition for use therein197116
US 3,788,958 AAqueous electrolytic stripping bath197413
US 3,935,005 AComposition and method for stripping gold and silver197615
US 4,056,450 AContinuous detinning system197712
US 4,078,918 AMethod for precious metal recovery197822
US 4,229,270 AProcess for the recovery of metal values from anode slimes198047
US 4,374,008 AProcess for separating tungsten from coinage metals198316
US 4,426,225 AGold recovery method198423
US 4,456,473 AMethod of making silver powder198412
US 4,456,474 AMethod of making fine silver powder198416
US 4,606,797 AMethod for recovery of high grade gold alloy from karat gold-clad base metal substrates198622
US 4,663,005 AElectropolishing process198766
US 4,678,552 ASelective electrolytic stripping of metal coatings from base metal substrates198735
EP 0,363,314 A1Process and device for recovering catalyst constituents—23
US 5,098,534 AComposition and method for electrolytically stripping silver19929
US 5,433,893 AConductive compositions199527
US 5,491,247 APreparation of a precious metal salt of a nonoxidizing acid by direct reaction19969
JP H0841676 ANon-cyan noble metal plating bath—18
US 5,728,854 AMethod for separating iron from nickel and/or cadmium from a waste containing the same19985
US 5,846,288 AElectrically conductive material and method for making199831
WO 9,945,158 A1Gold recovery process—10
US 5,963,772 AElectrically conductive material and method of making19998
US 6,129,779 AReclaiming metallic material from an article comprising a non-metallic friable substrate200052

Non-Patent Literature (5)

  • [No Author Listed] Lutropur MSA, Lutropur MSA 100. The “green” acid for use in cleaners. BASF, EMV 0113-00 e08.2008 . 16 pages.
  • [No Author Listed], Eco-Goldex Internet Home Page. Quebec, Canada. Available Aug. 31, 2016. Last accessed Mar. 3, 2017 from <http://www.eco-goldex.com/>. 2 pages.
  • [No Author Listed], Revolutionary New Processes for Stripping Precious Metals. Greene Lyon Group Press Release. Aug. 2014.
  • [No Author Listed], UWin Nanotech Co., Ltd. Internet Home Page. Taiwan. Available Nov. 9, 2012. Last accessed Mar. 3, 2017 from <http://uwin-nano.com/>. 1 page.
  • CN 201580010231.3, Feb. 24, 2018, Office Communication.