Degradable resin molding and production method for degradable resin molding
Abstract
Disclosed is a degradable film (1) in which a barrier layer (3) is disposed on a surface of a water-soluble polymer layer (2). The water-soluble polymer layer (2) is made of a water-soluble polymer such as polyvinyl alcohol or polyvinyl pyrrolidone. The barrier layer (3) is made of silicon oxide or silicon oxynitride. The barrier layer (3) is formed on the water-soluble polymer layer (2) by a CVD process with the supply of a raw material gas containing a precursor of a substance that forms the barrier layer (3), an ozone gas with an oxygen concentration of 20 vol % or higher and an unsaturated hydrocarbon gas to the water-soluble polymer layer (2).
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A production method of a degradable resin molded article, the degradable resin molded article having a barrier layer disposed on a surface of a water-soluble polymer layer, the water-soluble polymer layer containing polyvinyl alcohol or polyvinyl pyrrolidone, the barrier layer being a silicon oxide film or a silicon oxynitride film, the production method comprising: placing the water-soluble polymer layer in a vacuum chamber; and supplying, to the water-soluble polymer layer placed in the vacuum chamber, an ozone gas with an ozone concentration of 20 vol % or higher, a raw material gas contain
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (18)
Non-Patent Literature (2)
- Japanese Office Action and English translation, Application No. 2018-225082, dated Oct. 8, 2019, 8 pages.
- Kameda et al., Properties of a CVD-SiO2 Film at Room Temperature by Active Species from High Purity Ozone Gas, Japan Society of Applied Physics, Extended Abstracts of the 79th JSAP Autumn Meeting, 2018, 1 page.