Patents
US 11,549,181 B2#61372927 Most CitedActiveUnited States (USPTO)Utility

Methods for atomic layer deposition of SiCO(N) using halogenated silylamides

1Forward Citations (#61372927 Global)
0.3/yrCitation Velocity (#24715749 Global)
0.75Citation PageRank (#61372927 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Methods for the formation of films comprising Si, C, O and N are provided. Certain methods involve sequential exposures of a hydroxide terminated substrate surface to a silicon precursor and an alcohol-amine to form a film with hydroxide terminations. Certain methods involved sequential exposures of hydroxide terminated substrate surface to a silicon precursor and a diamine to form a film with an amine terminated surface, followed by sequential exposures to a silicon precursor and a diol to form a film with a hydroxide terminated surface.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of depositing a film comprising Si, C, O and N, the method comprising: exposing a substrate surface to a silicon precursor to form a film with silicon-halogen terminations, wherein the silicon precursor comprises a halogenated silyl amide, the silicon precursor comprises a compound having the general formula X n Si(NRR′) (4-n) , where n is 1-3, each X is independently F, Cl, Br or I, each of R and R′ is an alkyl having in the range of 5 to 8 carbon atoms or an aryl having in the range of 1 to 8 carbon atoms; and exposing the film with silicon-halogen terminations to an alcohol-amine t

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the silicon precursor comprises substantially no Si—C bonds.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein each X is selected from Br or I.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 5,074,017 ASusceptor199163
US 5,186,718 AStaged-vacuum wafer processing system and method1993640
US 5,580,388 AMulti-layer susceptor for rapid thermal process reactors199681
US 6,634,314 B2Atomic layer deposition method and semiconductor device fabricating apparatus having rotatable gas injectors2003120
US 2004004859 A1Memory utilizing oxide nanolaminates—56
US 6,818,250 B2Method for forming SIO2 by chemical vapor deposition at room temperature200441
US 2005025885 A1Low-temperature silicon nitride deposition—83
US 2005163927 A1Forming a silicon nitride film—64
US 2006102081 A1Wafer Guide, MOCVD Equipment, and Nitride Semiconductor Growth Method—49
US 7,244,683 B2Integration of ALD/CVD barriers with porous low k materials200725
US 2007218702 A1Semiconductor-processing apparatus with rotating susceptor—153
US 2008160174 A1Monosilane or disilane derivatives and method for low temperature deposition of silicon-containing films using the same—18
WO 2009/055340 A1Methods for forming a silicon oxide layer over a substrate—12
US 2009137132 A1Decreasing the etch rate of silicon nitride by carbon addition—8
WO 2009/149167 A2Low temperature deposition of silicon-containing films—18
US 2010068894 A1Composition and method for low temperature chemical vapor deposition of silicon-containing films including silicon carbonitride and silicon oxycarbonitride films—7
US 2010124618 A1Method of Forming Insulation Film Using Plasma Treatment Cycles—72
US 2010304047 A1Low Temperature Deposition of Silicon-Containing Films—28
US 7,897,208 B2Low temperature ALD SiO220119
US 2012009802 A1Plasma activated conformal dielectric film deposition—105
US 2012214318 A1Method of Depositing Dielectric Film by ALD Using Precursor Containing Silicon, Hydrocarbon, and Halogen—29
US 8,329,599 B2Method of depositing dielectric film by ALD using precursor containing silicon, hydrocarbon, and halogen201227
US 2013071580 A1Activated Silicon Precursors For Low Temperature Deposition—34
US 2013078376 A1Metal nitride containing film deposition using combination of amino-metal and halogenated metal precursors—36
US 2013118407 A1Substrate susceptor and deposition apparatus having same—23
TW 201,327,679 APlasma activated conformal dielectric film deposition—7
US 2013244446 A1Method for Forming Si-Containing Film Using Two Precursors by ALD—29
US 8,562,746 B2Sectional wafer carrier20138
US 2014273528 A1Si PRECURSORS FOR DEPOSITION OF SiN AT LOW TEMPERATURES—62

Non-Patent Literature (5)

  • “Non-Final Office Action in U.S. Appl. No. 16/550,486, dated May 27, 2021, 7 pages”.
  • “PCT International Search Report and Written Opinion in PCT/US2020/051509 dated Dec. 10, 2020, 9 pages”.
  • Ahn, Dongjoon , et al., “Thermodynamic measurements pertaining to the hysteretic intercalation of lithium in polymer-derived silicon oxycarbide” Journal of Power Sources 195 (2010) 3900-3906.
  • Closser, Richard G., et al., “Molecular Layer Deposition of a Highly Stable Silicon Oxycarbide Thin Film Using an Organic Chlorosilane and Water”. ACS Appl. Mater. Interfaces 2018, 10, 24266-24274.
  • Du, Y. , et al., “Mechanism of Pyridine-Catalyzed SiO2 Atomic Layer Deposition Studied by Fourier Transform Infrared Spectroscopy”, J. Phys. Chem. C vol. 111, 2007, 219-226.