Patents
US 11,548,817 B2#103271874 Most CitedActiveUnited States (USPTO)Utility

Method for the manufacture of mineral wool products with a phenol-formaldehyde resole based binder

0Forward Citations (#103271874 Global)
0.0/yrCitation Velocity (#103271874 Global)
0.56Citation PageRank (#103271874 Global)
15Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for the manufacture of mineral wool, is disclosed. In one example, the method comprises reacting an aqueous phenol-formaldehyde resole with free formaldehyde with a first amount of urea, thereby preparing a prereact; contacting the prereact with a second amount of urea; applying the resulting mixture of prereact and second amount of urea, as part of a binder, optionally with additives, to the surface of mineral fibers; and curing the binder on the surface of the mineral fibers. The total amount of urea used ranges 10-40 wt. % relative to the sum of the dry weight of the phenol-formaldehyde resole and the total amount of urea, and the second amount of urea used is at least 40 wt.-% of the total amount of urea. The invention also relates to a mineral wool product with reduced emissions of formaldehyde obtained by the method.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for the manufacture of mineral wool comprising: a) providing an aqueous phenol-formaldehyde resole having a free formaldehyde content of not more than 6% by weight, and less than 1% nitrogen by weight, b) preparing a phenol-formaldehyde-urea prereact by contacting the resole with a first amount of urea to form a first mixture and allowing the first mixture to react for at least one hour at a temperature in the range of 20-60° C.; wherein the first amount of urea ranges from 5-20 wt.% related to the sum of the dry weight of the phenol-formaldehyde resole and a total amount of urea used

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (15)

PatentTitleYearCitations
US 2,748,101 AWater-soluble phenol-formaldehyde condensation products195612
US 3,932,334 ACalcia catalyzed resins197621
JP S60139715 AResin for sizing composition, manufacture and sizing composition—5
US 4,663,419 APhenol-hcho-urea resin for a sizing composition, a process for its perparation and the sizing composition obtained198721
EP 0,253,488 A2Water soluble phenolic resole-urea composition—20
US 4,904,516 APhenol-formaldehyde resin solution containing water soluble alkaline earth metal salt199028
US 5,538,761 AProcess for preparing binder-treated fiberglass exhibiting lowered formaldehyde and ammonia emissions and product prepared thereby199635
WO 0,196,254 A1Insulating product in particular thermal containing a binder based on phenol-formaldehyde resin and method for making same—32
US 6,342,271 B1Phenolic resin for glue sizing composition, preparation method and glue sizing composition containing same20027
US 6,893,579 B2Insulation product in particular thermal containing a binder based on phenol-formaldehyde resin and method for making same20057
US 2007191574 A1Low Formaldehyde Emission Fiberglass—16
WO 2013/057432 A1Sizing composition having a low formaldehyde content for fire-resistant mineral wool and insulation product obtained—8
EP 2,657,266 A1Process for the preparation of a phenol-formaldehyde resin having a low amount of free formaldehyde, a phenol-formaldehyde resin resulting from this process, and the use of this resin as a binder for mineral wool insulation products—6
JP 2015527431 Aホルムアルデヒド不含のバインダーおよびミネラルウール断熱製品—4
US 9,242,899 B2Formaldehyde-free binder and use for mineral wool insulation products20165

Non-Patent Literature (1)

  • International Search Report in parallel PCT Application No. PCT/EP2017/077482 dated Feb. 6, 2018.