Patents
US 11,542,162 B2#38594048 Most CitedActiveUnited States (USPTO)Utility

Highly reactive, dust-free and free-flowing lithium sulphide and method for the production thereof

2Forward Citations (#38594048 Global)
0.7/yrCitation Velocity (#11879875 Global)
1.05Citation PageRank (#38752305 Global)
11Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a highly reactive, high-purity, free-flowing and dust-free lithium sulfide powder having an average particle size between 250 and 1,500 μm and BET surface areas between 1 and 100 m2/g. The invention, furthermore, relates to a process for its preparation, wherein in a first step, lithium hydroxide monohydrate is heated in a temperature-controlled unit to a reaction temperature between 150° C. and 450° C. in the absence of air, and an inert gas is passed over or through it, until the residual water of crystallization content of the formed lithium hydroxide is less than 5 wt. % and in a second step, the anhydrous lithium hydroxide formed in the first step is mixed, overflowed or traversed by a gaseous sulfur source from the group consisting of hydrogen sulfide, elemental sulfur, carbon disulfide, mercaptans or sulfur nitrides.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 2.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A lithium sulfide powder, characterized in that it has an average particle size between 250 and 1,500 μm and BET surface areas between 1 and 100 m 2 /g, and contains cationic impurities from the group consisting of alkali metal, alkaline earth metal and transition metal cations in the 0.01-100 ppm range, and anionic impurities from the group consisting of oxoanions of carbon and sulfur, as well as halides in concentrations of 1-1,000 ppm.

  2. Claim 2Depends on #1

    A process for preparing a lithium sulfide powder according to claim 1 , characterized in that in a first step, lithium hydroxide monohydrate having an average particle size in the range of 150-2,000 μm is heated in a temperature-controlled unit to a reaction temperature between 150° C. and 450° C. in the absence of air, and an inert gas is flowed over or through it, until the residual wa

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • Chen et al.; “High Capacity All-Solid-State Cu-Li2S/Li6PS5Br/In Batteries”, Solid State Ionics, 2014, 262, pp. 183-187.
  • Hassoun et al., “A High-Performance Polymer Tin Sulfur Lithium Ion Battery”; Angew. Chem.. Int. Ed., 2010, 49, pp. 2371-2374, and Supporting Information (3 pages).
  • Lee et al., “Nanostructured Lithium Sulfide Materials for Lithium-Sulfur Batteries”, J. Power Sources, 2016, 323, pp. 174-188.