Method for manufacturing high-strength galvanized steel sheet
Abstract
Provided is a method for manufacturing a high-strength galvanized steel sheet. Heating in a first half of oxidizing treatment is performed at a temperature of 400° C. to 750° C. in an atmosphere having a particular O2 concentration and a particular H2O concentration, and heating in a second half of the oxidizing treatment is performed at a temperature of 600° C. to 850° C. in an atmosphere having a particular O2 concentration and a particular H2O concentration. Subsequently, heating in a heating zone for reduction annealing is performed to a temperature of 650° C. to 900° C. at a particular heating rate in an atmosphere having a particular H2 concentration and a particular H2O concentration with the balance being N2 and inevitable impurities, and soaking in a soaking zone for the reduction annealing is performed in an atmosphere having a particular H2 concentration and a particular H2O concentration with the balance being N2 and inevitable impurities.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 32 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for manufacturing a high-strength galvanized steel sheet, the method comprising performing an oxidizing treatment, reduction annealing, and a galvanizing treatment in this order on a steel sheet having a chemical composition containing, by mass %, C: 0.3% or less, Si: 0.1% to 2.5%, Mn: 0.5% to 3.0%, P: 0.100% or less, S: 0.0100% or less, and the balance being Fe and inevitable impurities, wherein heating in a first half of the oxidizing treatment is performed at a temperature of 400° C. or higher and 750° C. or lower in an atmosphere having an O 2 concentration of 1000 vol.ppm or mor
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (32)
Non-Patent Literature (5)
- Chinese Office Action for Chinese Application No. 201780065491.X, dated Jan. 12, 2021, with Concise Statement of Relevance of Office Action, 8 pages.
- Chinese Office Action with Search Report for Chinese Application No. 201780065491.X, dated Jul. 30, 2020, 11 pages.
- Extended European Search Report for European Application No. 17864391.2, dated Jun. 28, 2019, 9 pages.
- Fonstein; Advanced High Strength Sheet Steels; Aug. 14, 2015; Springer; p. 19-21 (Year: 2015).
- International Search Report and Written Opinion for International Application No. PCT/JP2017/033180, dated Oct. 2, 2017, 6 pages.