Abstract

Provided is a high-strength steel sheet including, in % weight, carbon (C): 0.04 to 0.15%, silicon (Si): 0.01 to 1.0%, manganese (Mn): 1.8 to 2.5%, molybdenum (Mo): 0.15% or less (excluding 0%), chromium (Cr): 1.0% or less (excluding 0%), phosphorus (P): 0.1% or less, sulfur (S): 0.01% or less, aluminum (Al): 0.01 to 0.5%, nitrogen (N): 0.01% or less, boron (B): 0.01% or less (excluding 0%), antimony (Sb): 0.05% or less (excluding 0%), one or more of titanium (Ti): 0.003 to 0.06% and niobium (Nb): 0.003 to 0.06%, a balance of Fe and other unavoidable impurities, and contents of the C, the Si, the Al, the Mo and the Cr satisfy the following Expression 1: Expression 1: {(2×(Si+Al))+Mo+Cr}/C≥15. The high-strength steel sheet comprises: a ferrite phase, a bainite phase, a martensite phase, and a residual austenite phase, the ferrite phase being less than 40% of area fraction in the microstructure.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 48 · Forward citations: 0.

Claims (5)

  1. Claim 1Independent Claim

    A steel sheet comprising, in % weight, carbon (C): 0.04 to 0.15%, silicon (Si): 0.01 to 0.6%, manganese (Mn): 1.8 to 2.5%, molybdenum (Mo): 0.15% or less (excluding 0%), chromium (Cr): 1.0% or less (excluding 0%), phosphorus (P): 0.1% or less, sulfur (S): 0.01% or less, aluminum (Al): 0.01 to 0.5%, nitrogen (N): 0.01% or less, boron (B): 0. 01% or less (excluding 0%), antimony (Sb): 0.01 to 0.05%, one or more of titanium (Ti): 0.003 to 0.06% and niobium (Nb): 0.003 to 0.06%, a balance of Fe and other unavoidable impurities, and contents of the C, the Si, the Al, the Mo and the Cr satisfying the following Expression 1 and contents of the Si, the Al, the Mo, the Cr and the C in the ferrite phase satisfy the following Expression 2: Expression 1 {(2x(Si+Al))+Mo+Cr}/C≥15 (where Si refers to a content of the Si in % weight, Al refers to a content of the Al in % weight, Mo refers to a content of the Mo in % weight, Cr refers to a content of the Cr in % weight, and C refers to a content of the C in % weight), Expression 2 {(2x(Si F +Al F ))+Mo F +Cr F }/C F ≥500 (where Si F refers to a content of the Si in % weight, Al F refers to a content of the Al in % weight, Mo F refers to a content of the Mo in % weight, Cr F refers to a content of the Cr in % weight, and C F refers to a content of the C in % weight), wherein the steel sheet comprises: a microstructure including a ferrite phase, a bainite phase, a martensite phase, and a residual austenite phase, the ferrite phase being 31% to 40% of area fraction in the microstructure, and wherein an area ratio (Fn/Ft) of non-recrystallized ferrite (Fn) in the ferrite phase (Ft) is 20% or less (including 0%).

  2. Claim 2Depends on #1

    The steel sheet of claim 1 , wherein a hardness ratio of the martensite phase, the bainite phase and the ferrite phase satisfies the following Expression 3: Expression 3 (H B +H M )/(2xH F )≤3 (where H B refers to a hardness of bainite phase, H M refers to a hardness of martensite phase, and H F refers to a hardness of ferrite phase).

  3. Claim 3Depends on #1

    The steel sheet of claim 1 , wherein the steel sheet further comprises: a hot dipped galvanized layer formed on at least one surface thereof.

  4. Claim 4Depends on #1

    The steel sheet of claim 1 , wherein the steel sheet has a tensile strength of 980 MPa or more, a three-point bending angle is 80 degrees or more, and a product (YSxEl) of yield strength and elongation is 10000 or more.

  5. Claim 5Independent Claim

    A steel sheet comprising, in % weight, carbon (C): 0.04 to 0.15%, silicon (Si): 0.01 to 0.6%, manganese (Mn): 1.8 to 2.5%, molybdenum (Mo): 0.15% or less (excluding 0%), chromium (Cr): 1.0% or less (excluding 0%), phosphorus (P): 0.1% or less, sulfur (S): 0.01% or less, aluminum (Al): 0.01 to 0.5%, nitrogen (N): 0.01% or less, boron (B): 0. 01% or less (excluding 0%), antimony (Sb): 0.01 to 0.05%, one or more of titanium (Ti): 0.003 to 0.06% and niobium (Nb): 0.003 to 0.06%, a balance of Fe and other unavoidable impurities, and contents of the C, the Si, the Al, the Mo and the Cr satisfying the following Expression 1: Expression 1 {(2x(Si+Al))+Mo+Cr}/C≥15 (where Si refers to a content of the Si in % weight, Al refers to a content of the Al in % weight, Mo refers to a content of the Mo in % weight, Cr refers to a content of the Cr in % weight, and C refers to a content of the C in % weight), wherein the steel sheet comprises: a microstructure including a ferrite phase, a bainite phase, a martensite phase, and a residual austenite phase, the ferrite phase being 31% to 40% of area fraction in the microstructure, and wherein contents of the Si, the Al, the Mo, the Cr and the C in the ferrite phase satisfy the following Expression 2: Expression 2 {(2x(Si F +Al F ))+Mo F +Cr F }C F ≥500 (where Si F refers to a content of the Si in % weight, Al F refers to a content of the Al in % weight, Mo F refers to a content of the Mo in % weight, Cr F

Technical Overview & Description

TECHNICAL FIELD The present invention relates to a high-strength steel sheet used for an automotive structural member, and more particularly, to a high-strength steel sheet with excellent crashworthiness characteristics and formability and a method for manufacturing the same. BACKGROUND ART In the automotive industry, regulations on carbon dioxide emissions as well as environmental and safety regulations have become increasingly severe, and fuel regulations for automobiles are also being tightened. In addition, the US Highway Safety Insurance Association is increasingly regulating collision safety to protect passengers, and requires severe crash performance, such as a 25% overlap from 2013 regulations. Research to reduce the weight of automobiles as a means of solving the problems in the automobile industry is being carried out continuously. Generally, high-strength automobile materials can be classified into a precipitation hardening steel, a bake hardenable steel, a solid solution strengthening steel, a transformed hardened steel, etc. In the transformed hardened steel among them, dual phase steel (DP steel), transformation induced plasticity steel (TRIP steel), complex phase steel (CP steel) and the like are included. Such transformed hardened steel is called advanced high strength steel (AHSS). DP steel is a steel in which hard martensite is finely and homogeneously dispersed in soft ferrite to ensure high strength. CP steel contains two or three phases of ferrite, martensite and bainite, and includes precipitation hardening elements such as Ti, Nb and the like to enhance strength. TRIP steel is a type of steel capable of securing high strength and high ductility, causing martensite transformation when remaining fine austenite, which is homogeneously dispersed, is processed at room temperature. Meanwhile, recently, a steel sheet for automobiles has required even higher strength to improve fuel economy or durability

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (48)

PatentTitleYearCitations

Non-Patent Literature (8)

  • Chinese Office Action—Chinese Application No. 201880082866.8 dated Mar. 19, 2021, citing CN 101960034, CN 101910439, KR 10-2013-0160142, CN 102046827, CN 102414335, CN 105734411, CN 106062232, CN 107164695, CN 1310770, and JP 2005-154872.
  • European Search Report—European Application No. 18890761.2 dated Aug. 17, 2020, citing EP 2256224, EP 2123786, US 2011/017363, US 2017/260602, EP 2426230, US 2016/186282, JP 5865516, KR 10-0711468, WO 2017/155263, CA 2990356, and EP 2559782.
  • International Search Report—PCT/KR2018/011679 dated Jan. 23, 2019.
  • Japanese Office Action—Japanese Application No. 2020-529243 dated Feb. 1, 2022, citing JP 4860782, JP 5320681, JP 2010-275628, CN 105734410, JP 2011-508085, JP 2015-507094, WO 2017/131054, and JP 2009-51841.
  • Japanese Office Action—Japanese Application No. 2020-529243 dated Jun. 1, 2021, citing JP 2010-275628, CN 105734410, JP 2011-508085, JP 2015-507094, WO 2017/131054, and JP 2009-51841.
  • NPL: English on-line translation of KR 20130106142 A, Sep. 2013 (Year: 2013).
  • NPL: On-line English translation of CN 105734410 A, Jul. 2016 (Year: 2016).
  • NPL: Pande et al, Impurities in commercial ferroalloys and its influence on the steel cleanliness, Applications and Uses, The twelfth international Ferroalloys congress, Jun. 2010, pp. 935-944 (Year: 2010).