Abstract

A polyethylene composition including a first polyethylene which is an ethylene copolymer having a weight average molecular weight of from 70,000 to 250,000 and a molecular weight distribution M w /M n of <2.3, a second polyethylene which is an ethylene copolymer or homopolymer having a weight average molecular weight of less than 75,000 and a molecular weight distribution M w /M n of <2.3, and a third polyethylene which is an ethylene copolymer or homopolymer having a weight average molecular weight of from 100,000 to 300,000 and a molecular weight distribution M w /M n of >2.3, where the first polyethylene has more short chain branching than the second polyethylene or the third polyethylene. The polyethylene composition has a soluble fraction in a CEF analysis of at least 15 weight percent. A film made from the polyethylene composition may have a machine direction 1% secant modulus of ≥200 MPa (at a film thickness of about 1 mil) and an oxygen transmission rate (OTR) of ≥700 cm 3 per 100 inch 2 per day (at a film thickness of about 1 mil). A film made from the polyethylene composition retains much of its dart impact performance on downgauging from a thickness of 1 mil to

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A polyethylene composition comprising: from 15 to 75 wt % of a first polyethylene which is an ethylene copolymer, the first polyethylene having a weight average molecular weight Mw of from 70,000 to 250,000, a molecular weight distribution M w /M n of <2.3 and from 5 to 100 short chain branches per thousand carbon atoms; from 5 to 80 wt % of a second polyethylene which is an ethylene copolymer or an ethylene homopolymer, the second polyethylene having a weight average molecular weight Mw of less than 75,000, a molecular weight distribution M w /M n of <2.3 and from 0 to 20 short chain

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (22)

PatentTitleYearCitations
WO 9,426,816 A1Ethylene copolymers having narrow composition distribution, their production and use—99
US 5,376,439 ASoft films having enhanced physical properties1994202
WO 9,820,062 A1Films useful in the modified atmosphere packaging of perishable food—26
US 6,114,486 ARheology-modified polyolefins2000113
WO 03,074,594 A1Film suitable for food packaging—22
US 2003213938 A1Metallocene-produced very low density polyethylenes—43
US 2008038533 A1Linear polymers, polymer blends, and articles made therefrom—94
WO 2008/077530 A2Multimodal polyethylene composition, mixed catalyst and process for preparing the composition—36
US 2008306216 A1Adhesive and coating compositions—23
US 2009297810 A1Polyethylene Films and Process for Production Thereof—64
US 2011040041 A1Polymerization Processes Using Metallocene Catalysts, Their Polymer Products and End Uses—21
US 8,022,143 B2Closures for bottles201161
WO 2014/099307 A1Branched polyethylene with improved processing and high tear films made therefrom—38
US 2016108221 A1Solution polymerization process—28
WO 2017/106120 A2Multilayer films suitable for use in thermoforming applications—22
US 9,963,529 B1Multi reactor solution polymerization201854
US 2018305531 A1Means For Increasing the Molecular Weight and Decreasing the Density of Ethylene Interpolymers Employing Homogeneous and Heterogeneous Catalyst Formulations—43
WO 2019/126845 A1Composition for use in rotational moulding processes and use of the composition—10
WO 2019/132694 A1Polyethylene composition—26
WO 2019/133394 A1Compositions comprising multimodal ethylene based polymers and low density polyethylene (ldpe)—16
US 2020165366 A1Films Made from Polyethylene Compositions and Processes for Making Same—9
US 2021079138 A1Dual reactor solution process for the production of multimodal ethylene-based polymer—7

Non-Patent Literature (5)

  • ASTM D1003-13—Standard Test Method for Haze and Luminous Transmittance of Transparent Plastics—Copyright ASTM International—Current edition approved Nov. 15, 2013. Published Nov. 2013. Originally approved in 1949. Last previous edition approved in 2011 as D1003-11. pp. 1-7.
  • ASTM D1238-13—Standard Test Method for Melt Flow Rates of Thermoplastics by Extrusion Plastometer—Copyribht ASTM International—Current edition approved Aug. 1, 2013. Published Aug. 2013. Originally approved in 1965. Last previous edition approved in 2010 as D1238-10. 1-16.
  • ASTM D1709-09—Standard Test Methods for Impact Resistance of Plastic Film by the Free-Falling Dart Method—Copyright ASTM International—Current edition approved May 1, 2009. Published Jun. 2009. Originally approved in 1959. Last previous edition approved in 2008 as D1709-08. pp. 1-9.
  • ASTM D1922-09—Standard Test Method for Propagation Tear Resistance of Plastic Film and Thin Sheeting by Pendulum Method—Copyright ASTM International—Current edition approved May 1, 2009. Published Jun. 2009. Originally approved in 1961. Last previous edition approved in 2008 as D1922-08. pp. 1-7.
  • ASTM D2457-13—Standard Test Method for Specular Gloss of Plastic Films and Solid Plastics—Copyright ASTM International—Current edition approved Apr. 1, 2013. Published Apr. 2013. Originally approved in 1965. Last previous edition approved in 2008 as D2457-08. pp. 1-6.