Patents
US 11,267,017 B2#67233659 Most CitedActiveUnited States (USPTO)Utility

Method for applying ultraviolet curable coating material and method for producing ultraviolet cured film

0Forward Citations (#67233659 Global)
0.0/yrCitation Velocity (#67233659 Global)
0.56Citation PageRank (#67233659 Global)
29Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for applying an ultraviolet curable coating material and a method for producing an ultraviolet cured film include the steps of: supplying an ultraviolet curable coating material containing an ultraviolet curable acrylic monomer into a mixer under a condition of greater than or equal to 8 MPa without diluting the ultraviolet curable coating material with an organic solvent; supplying carbon dioxide with a critical pressure or more into the mixer; mixing the ultraviolet curable coating material and the carbon dioxide supplied into the mixer to form a mixed fluid; spraying the mixed fluid under a condition of a critical pressure or more of the carbon dioxide to form a coating film; and irradiating the coating film with ultraviolet rays to form an ultraviolet cured film.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for applying an ultraviolet curable coating material, the method comprising the steps of: supplying an ultraviolet curable coating material containing an ultraviolet curable acrylic monomer into a mixer under a condition of greater than or equal to 8 MPa without diluting the ultraviolet curable coating material with an organic solvent; supplying carbon dioxide with a critical pressure or more into the mixer; mixing the ultraviolet curable coating material and the carbon dioxide supplied into the mixer to form a mixed fluid; spraying the mixed fluid under a condition of a critical pres

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (29)

PatentTitleYearCitations
US 4,506,682 AClear tobacco aroma oil, a process for obtaining it from a tobacco extract, and its use1985381
JP H01258770 ASupercritical fluid as diluent in liquid spray coating of film—21
US 5,009,367 AMethods and apparatus for obtaining wider sprays when spraying liquids by airless techniques1991125
US 5,027,742 ASupercritical fluids as diluents in liquid spray application of coatings199174
US 5,171,613 AApparatus and methods for application of coatings with supercritical fluids as diluents by spraying from an orifice199295
JP H0568936 ARelease sheet and production thereof—7
US 5,197,800 AMethod for forming coating material formulations substantially comprised of a saturated resin rich phase199354
US 5,203,843 ALiquid spray application of coatings with supercritical fluids as diluents and spraying from an orifice199324
US 5,211,342 AElectrostatic liquid spray application of coatings with supercritical fluids as diluents and spraying from an orifice199364
JP H05277429 APolyester particularly suitable for use in coating composition which is sprayed with compressed fluid as viscosity reducing agent—6
US 5,362,519 APolyesters particularly suitable for use in coating compositions which are sprayed with compressed fluids as vicosity reducing agents199426
US 5,443,796 AMethod and apparatus for preventing the formation of a solid precipitate in a coating material formulation199515
WO 2004/108844 A2Dual radiation/thermal cured coating composition—10
JP 2006526688 A放射線/熱による二重硬化塗料組成物—6
JP 2008012453 AHigh-temperature high-pressure micromixer—35
WO 2010/113489 A1Carbon dioxide coating method and device therefor—18
JP 2010234349 AMethod of applying one-pack type or two-pack type coating material using carbon dioxide and device using this method—10
JP 2010234348 ACarbon dioxide coating method and device therefor—18
US 2012097751 A1Carbon dioxide coating method and device therefor—3
JP 2012086150 AMethod for carbon dioxide coating and device for the same—26
JP 2012086151 AMethod for carbon dioxide coating and device for the same—15
JP 2012086175 ACoating film formation method and coating film—19
JP 2012224700 AMethod for producing non-spherical resin particulate—4
JP 2013189545 ASolvent-free ultraviolet-curable resin composition—14
US 8,864,044 B2Carbon dioxide coating method and device therefor20141
JP 2014223599 ACoating method of low viscosity coating material—6
JP 5,923,677 B1コーティング液組成物、コーティング膜の形成方法、コーティング液組成物の製造方法、コーティング液組成物の製造装置、及び、二酸化炭素含有コーティング液組成物調製用組成物201614
JP 5,972,435 B1コーティング液組成物、コーティング液組成物の製造方法、及び、コーティング液組成物調製用組成物20164
JP 6,006,448 B1塗装装置20166

Non-Patent Literature (5)

  • Japanese Patent Office, International Search Report in International Patent Application No. PCT/JP2016/074477 (dated Nov. 15, 2016).
  • Japanese Patent Office, Notice of Grounds of Rejection in Japanese Patent Application No. 2016-029686 (dated Jan. 7, 2020).
  • Kawasaki, “‘Green’ Spray Coating Technology Using High Pressure CO2 for Diluent,” Journal of the Institute of Electrostatics Japan, 39(3): 116-120 (2015).
  • Korean Intellectual Property Office, Office Action in Korean Patent Application No. 10-2018-7024265 (dated May 4, 2020).
  • Suzuki et al., “Development of carbon dioxide coating technology using high-pressure micromixer,” Journal of Japan Coating Technology Association, 44(7): 230-238 (2009).