Tempered glass

0Forward Citations (#115379518 Global)
0.0/yrCitation Velocity (#115379518 Global)
0.56Citation PageRank (#115379518 Global)
29Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A tempered glass has a sheet thickness of 0.6 mm or less and having a compression stress layer resulting from chemical tempering at a surface thereof, which satisfies requirements of CS×(DOL−20)/DOL>360 and DOL/t≤0.20 when the compression stress value of the compression stress layer is represented by CS (Mpa), the depth of the compression stress layer is represented by DOL (μm), and the sheet thickness is represented by t (μm).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A tempered glass having a sheet thickness of less than 0.5 mm and a compression stress layer subjected to chemical tempering at a surface of the tempered glass, which satisfies CS≥670, 360<CS×(DOL−20)/DOL≤430, DOL/t≤0.20, and 85≤CT≤109.2, wherein CS (Mpa) represents a compression stress value caused by the compression stress layer, DOL (μm) represents a depth of the compression stress layer, t (μm) represents a sheet thickness of the compression stress layer, and CT (MPa) represents an internal tensile stress value of the compression stress layer.

  2. Claim 2Depends on #1

    The tempered glass according to claim 1 , wherein the compression stress value is from 670 to 1,200 MPa and the depth of the compression stress layer is from 25 to 60 μm.

  3. Claim 3Depends on #1

    The tempered glass according to claim 1 , which is subjected to chemical tem

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (29)

PatentTitleYearCitations
JP H11328601 AGlass board for recording medium, recording medium using glass board and manufacture of glass board for recording medium—73
US 2008286548 A1Down-drawable, chemically strengthened glass for cover plate—161
US 2009197088 A1Tempered glass substrate and method of producing the same—170
JP 2010116276 ATempered glass substrate and producing method of the same—67
CN 101,772,470 ATempered glass substrate and method for producing same—30
JP 2010527892 Aダウンドロー法で製造可能な、化学的に強化されたカバープレート用ガラス—45
WO 2011/114821 A1Glass composition for chemical strengthening and chemically strengthened glass material—34
JP 2011213576 AGlass composition for chemical strengthening, and chemically strengthened glass material—68
WO 2013/051514 A1Cover glass—9
TW 201,315,692 ACover glass—1
JP 5,293,908 B1ディスプレイ用カバーガラス、ディスプレイ用カバーガラスの製造方法20133
WO 2013/191110 A1Support member for contactless power supply—10
WO 2014/030738 A1Glass substrate for cover glass for electronic device, cover glass for electronic device, and method for manufacturing glass substrate for cover glass for electronic device—10
US RE44869 EDown-drawable, chemically strengthened glass for cover plate20146
CN 103,842,311 ACover glass—7
JP 2014141363 AChemically strengthenable glass, glass sheet, and chemically strengthened cover glass—35
WO 2014/189117 A1Method for manufacturing tempered glass sheet—6
US 2014370264 A1Display cover glass and display cover glass fabrication method—29
US 2015030834 A1Strengthened glass articles having improved survivability—98
WO 2015/080043 A1Glass member, and glass-member production method—30
US 2015239775 A1Strengthened glass with deep depth of compression—86
WO 2015/178175 A1Tempered glass plate and method for producing same—5
TW 201,600,475 ATempered glass plate and method for producing same—1
JP 2016000682 AStrengthened glass plate and production method thereof—6
US 2016083292 A1Method for manufacturing tempered glass sheet—11
US 2016102015 A1Method for producing toughened glass plate—5
US 2016318796 A1Glass member and manufacturing method of glass member—22
US 2018009706 A1Thin glass article with a non-uniformly ion-exchanged surface layer and method for producing such a thin glass article—6
JP 2018511550 A不均一にイオン交換された表面層を有する薄型ガラス物品およびこのような薄型ガラス物品を製造する方法—2

Non-Patent Literature (5)

  • CN Office Action dated Nov. 14, 2019 in Chinese Application No. 201680025340.7 (with attached English-language translation).
  • International Search Report dated Jun. 7, 2016 for PCT/JP2016/060023.
  • International Search Report/Written Opinion dated Jun. 7, 2016 for PCT/JP2016/060023 [Japanese language].
  • JP Office Action dated Dec. 10, 2019 from corresponding Japanese patent application No. 2017-514037 (with attached English-language translation).
  • JP Office Action dated Oct. 8, 2019 from corresponding Japanese patent application No. 2017-514037 (with attached English-language translation).