Methods for treating inner liner surface, inner liners resulting therefrom and tires containing such inner liners
Abstract
Methods for treating the surface of a cured inner liner are disclosed. By use of these methods a treated, cured inner liner is produced which has a lower surface with increased adherability to other materials (e.g., adhesives). Treated, cured inner liners resulting from such methods as well as tires containing the treated inner liners.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for treating the surface of a cured tire inner liner comprising: providing a cured tire inner liner having a thickness of 0.5 to 2 mm and an upper and a lower surface wherein the tire inner liner comprises rubber, a majority by weight of which comprises butyl rubber, and 10-100 phr of at least one filler comprising carbon black, clay, or silica, and the lower surface further comprises polysiloxane moieties, and treating the lower surface of the cured tire inner liner to convert at least a portion of the polysiloxane moieties to silanol moieties, thereby producing a treated, cured tire
- Claim 2Depends on #1
The method of claim 1 , wherein the treating comprises exposing the lower surface of the cured tire inn
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗