Method for preparing graphene by liquid-phase ball milling exfoliation
Abstract
Provided is a method for preparing graphene by liquid-phase ball milling exfoliation, including following steps: mixing a transition metal halide salt, a nitrogen source substance and an organic solvent to prepare an intercalation agent; mixing the intercalation agent with graphite, carrying out ball milling, and then performing centrifugation to obtain a graphite intercalation compound; washing and filtering the graphite intercalation compound obtained, adding an expansion agent, and carrying out ultrasonic agitation to obtain a graphene dispersion; and washing, filtering and drying the graphene dispersion to obtain graphene powder.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 1.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for preparing graphene by liquid-phase ball milling exfoliation, comprising following steps: mixing a transition metal halide salt, a nitrogen source substance and an organic solvent to prepare an intercalation agent; mixing the intercalation agent obtained with graphite, carrying out ball milling, and then performing centrifugation to obtain a graphite intercalation compound; washing and filtering the graphite intercalation compound, adding an expansion agent, and carrying out ultrasonic agitation to obtain a graphene dispersion; and washing, filtering and drying the graphene dispers
- Claim 2Depends on #1
The method of claim 1 , wherein the mass ratio of the transition metal halide salt, the nitrogen source substance and the organic solvent is (1-10):1:(2-10).
- Claim 3Independent Claim
The method of claim
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| ES 2,978,435 R1 | Grafito expandido y método de preparación para el mismo | — | 0 |