Electrolyte formulations for electrochemical cells containing a silicon electrode
Abstract
Additives to electrolytes that enable the formation of comparatively more robust SEI films on silicon anodes. The SEI films in these embodiments are seen to be more robust in part because the batteries containing these materials have higher coulombic efficiency and longer cycle life than comparable batteries without such additives.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 86 · Forward citations: 0.
Claims (17)
- Claim 1Independent Claim
A method of forming a solid-electrolyte interphase on an anode in a lithium ion battery, comprising: charging and discharging the lithium ion battery to form the solid-electrolyte interphase, wherein the lithium ion battery comprises: (i) an anode comprising silicon; (ii) a cathode; and (iii) an electrolyte solution; wherein the electrolyte solution comprises a lithium salt, ethylene carbonate, and an organic additive selected from the group consisting of mono-(trimethylsilyl)phosphite, tris(trimethylsilyl)phosphite, tris(trimethylsilyl)phosphate, tris(trimethylsilyl)borate, tris(trimethylsiloxy)vinylsilane, tris(trimethylsilyl)silane, and tris(trimethylsiloxy) ethylene.
- Claim 2Depends on #1
The method of claim 1 wherein the battery is charged to at least 4.2 V.
- Claim 3Depends on #1
The method of claim 1 wherein the battery is charged to greater than 4.2 V.
- Claim 4Depends on #1
The method of claim 1 wherein the battery is charged to at least 4.45 V.
- Claim 5Depends on #1
The method of claim 1 wherein the battery is charged and discharged at least 200 times and the solid-electrolyte interphase remains stable as demonstrated by a capacity retention by the battery of at least 60% at cycle 200 .
- Claim 6Depends on #1
The method of claim 1 wherein the battery is charged and discharged at least 200 times and the solid-electrolyte interphase remains stable as demonstrated by a capacity retention by the battery of at least 70% at cycle 200 .
- Claim 7Depends on #1
The method of claim 1 wherein the battery is charged and discharged at least 200 times and the solid-electrolyte interphase remains stable as demonstrated by a capacity retention by the battery of at least 80% at cycle 200 .
- Claim 8Depends on #1
The method of claim 1 wherein the battery is charged and discharged at least 200 times and the solid-electrolyte interphase remains stable as demonstrated by a capacity retention by the battery of at least 90% at cycle 200 .
- Claim 9Depends on #1
The method of claim 1 wherein the organic additive comprises mono-(trimethylsilyl)phosphite.
- Claim 10Depends on #1
The method of claim 1 wherein the organic additive comprises tris(trimethylsilyl)phosphite.
- Claim 11Depends on #1
The method of claim 1 wherein the organic additive comprises tris(trimethylsilyl)phosphate.
- Claim 12Depends on #1
The method of claim 1 wherein the organic additive comprises tris(trimethylsilyl)borate.
- Claim 13Depends on #1
The method of claim 1 wherein the organic additive comprises tris(trimethylsiloxy)vinylsilane.
- Claim 14Depends on #1
The method of claim 1 wherein the organic additive comprises tris(trimethylsilyl)silane.
- Claim 15Depends on #1
The method of claim 1 wherein the organic additive comprises tris(trimethylsiloxy) ethylene.
- Claim 16Independent Claim
A method comprising: generating an electrolyte solution that comprises a lithium salt, ethylene carbonate, and an organic additive, wherein the organic additive contains at least one methylsiloxy functional group ((CH 3 ) 3 SiO—); constructing a lithium ion battery that comprises: (i) an anode comprising silicon; (ii) a cathode; and (iii) the electrolyte solution; and charging and discharging the lithium ion battery to form a solid-electrolyte interphase on the anode.
- Claim 17Depends on #16
The method of claim 16 , wherein the organic additive is selected from the group consisting of mono-(trimethylsilyl)phosphite, tris(trimethylsilyl)phosphite, tris(trimethylsilyl)phosphate, tris(trimethylsilyl)borate, tris(trimethylsiloxy)vinylsilane, and tris(trimethylsiloxy) ethylene.
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATIONS The present application is a continuation of and claims the benefit of U.S. non-provisional application Ser. No. 15/689,776 filed Aug. 29, 2017 entitled “Electrolyte Formulations for Electrochemical Cells Containing a Silicon Electrode”. The '776 application claims the benefit of priority to U.S. provisional patent application Ser. No. 62/381,323 filed Aug. 30, 2016 entitled “Electrolyte Formulations for Lithium Ion Batteries”. Both of the '776 and '323 applications are incorporated by reference herein in their entireties. STATEMENT REGARDING FEDERALLY SPONSORED RESEARCH OR DEVELOPMENT This invention was made with government support under DOE EE0006453 awarded by the Department of Energy. The government has certain rights in the invention. BACKGROUND OF THE INVENTION The present invention is in the field of battery technology and, more particularly, electrolyte formulations that address challenges encountered during the use of silicon anodes in lithium ion batteries. Lithium ion batteries enjoy relatively widespread use, but research continues into improving the energy density, capacity, and cycle life of these batteries. For example, silicon has been used as an anode material to improve the energy density of lithium ion cells. Silicon anodes can provide high energy density to lithium ion batteries due to the high theoretical capacity of silicon, which is 4200 mAh/g. However, the silicon particles that make up the anode can undergo larges changes in their volume during battery cycling. The volumetric changes on lithiation and delithiation cycles can be as large as about 300%. These large volumetric changes in the silicon anode material can have negative effects on battery cycle life. A number of mechanisms may contribute to poor cycle life. For example, silicon particles can fracture due to the large stresses in the material brought on by the large chang
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (86)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 6,797,437 B2 | Electrolyte system and energy storage device using same | 2004 | 1 |
Non-Patent Literature (10)
- Bouillon, Jean-Philippe et al., “Synthesis and Intramolecular Aldol Reactions of 1,6- and 1,7-Bis(acylsilanes)” European Journal of Organic Chemistry (1999) 1571-1580.
- Fisher, Craig A.J. et al., “Lithium Battery Materials LiMPO4 (M = Mn, Fe, Co, and Ni): Insights into Defect Association, Transport Mechanism, and Doping Behavior” Chemical Materials 2008, 20, 5907-5915.
- Goodenough, John B. et al., “Challenges for Rechargeable Li Batteries” Chemistry of Materials Review 2010, 22, 587-603.
- International Search Report & Written Opinion dated Dec. 6, 2017 in International application No. PCT/US2017/049111.
- Johnson, Christopher S. et al., “Synthesis, Characterization and Electrochemistry of Lithium Battery Electrodes: kLi2MnO3-(1-x)LiMn0.333Ni0.333Co0.333O2 (0<x<0.7)” Chemical Materials 2008, 20, 6095-6106.
- Kang, S.-H. et al., “Interpreting the structural and electrochemical complexity of 0.5Li2MnO3-0.5LiMO2 electrodes for lithium batteries” Journal of Materials Chemistry, 2007, 17, 2069-2077.
- Marom, Rotem et al., “A review of advanced and practical lithium battery materials” Journal of Materials Chemistry, 2011, 21, 9938.
- Nagahama, Masatoshi et al., “High Voltage Performances of Li2NiPO4F Cathode with Dinitrile-Based Electrolytes” Journal of the Electrochemical Society, 157 (6) A748-A752 (2010).
- Saleur, Damien et al., “First synthesis of 1 ,4-bis(acylsilanes)” Tetrahedron Letters 41 (2000) 321-324.
- Supplementary European Search Report dated Jun. 2, 2015 in European Patent application No. EP12796608.3.