Abstract

Known protective layers having a high Cr-content and a silicone in addition, form brittle phases that embrittle further under the influence of carbon during use. The protective layer according to the invention is composed of 22% to 26% cobalt (Co), 10.5% to 12% aluminum (Al), 0.2% to 0.4% Yttrium (Y) and/or at least one equivalent metal from the group comprising Scandium and the rare earth elements, 15% to 16% chrome (Cr), optionally 0.3% to 1.5% tantal, the remainder nickel (Ni).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 40 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A protective single layer for protecting a component against corrosion and/or oxidation, the component having a substrate which is nickel-based or cobalt-based and the single layer resides on the substrate, wherein the single layer has the composition of an alloy, which consists of: 22% wt % to 26% wt % cobalt (Co), 15% wt % to 16% wt % chromium (Cr), 10.5% wt % to 12% wt % aluminum (Al), at least 0.3% wt % of tantalum and a maximum of 1.5% wt % tantalum, a total of 0.2% wt % to 0.6% wt % of yttrium (Y), and the balance nickel (Ni), wherein no silicon precipitates are formed during use at leas

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (40)

PatentTitleYearCitations
US 4,005,989 ACoated superalloy article1977137
US 4,034,142 ASuperalloy base having a coating containing silicon for corrosion/oxidation protection1977128
US 4,326,011 AHot corrosion resistant coatings198231
WO 9,101,433 A1Dual alloy turbine blade—43
JP H0432546 AMethod for repairing moving blade of gas turbine—22
US 5,106,266 ADual alloy turbine blade199231
EP 0,892,090 A1Method for manufacturing single crystal structures—479
WO 9,923,279 A1High temperature protective coating—21
WO 9,967,435 A1Directionally solidified casting with improved transverse stress rupture strength—516
US 6,024,792 AMethod for producing monocrystalline structures2000687
WO 0,044,949 A1Nickel base superalloy with good machinability—510
RU 2,165,475 C2Method of protection of steel machine components from salt attack200114
US 6,231,692 B1Nickel base superalloy with improved machinability and method of making thereof200127
US 6,245,447 B1Iron aluminide coating and method of applying an iron aluminide coating20015
US 6,280,857 B1High temperature protective coating200139
EP 0,922,781 B1Iron aluminide coating and process for application of this iron aluminide coating20031
EP 1,306,454 A1Rhenium containing protective coating protecting a product against corrosion and oxidation at high temperatures—513
CA 2,414,019 A1High temperature-resistant component—10
EP 1,319,729 A1High temperature resistant part, made of single-crystal or polycrystalline nickel-base superalloy—523
US 6,610,419 B1Product with an anticorrosion protective layer and a method for producing an anticorrosion protective200354
US 2004011439 A1Directionally solidified casting with improved transverse stress rupture strength—24
US 2004079648 A1Method of depositing an oxidation and fatigue resistant MCrAIY-coating—19
EP 1,204,776 B1High-temperature part and method for producing the same2004489
US 2004180233 A1Product having a layer which protects against corrosion. and process for producing a layer which protects against corrosion—64
CN 1,198,964 CHigh temp. protective coating20057
US 6,924,046 B2Rhenium-containing protective layer for protecting a component against corrosion and oxidation at high temperatures200517
CN 1,665,959 AHighly oxidation resistant component—21
US 2005238907 A1Highly oxidation resistant component—22
US 2005238893 A1Highly oxidation resistant component—11
US 7,005,015 B2High-temperature-resistant component and process for producing the high-temperature-resistant component200616

Non-Patent Literature (5)

  • Chinese Office Action dated Apr. 11, 2016 in corresponding Chinese Patent Application No. 201280044329.7, along with an English translation of relevant portions thereof.
  • Chinese Office Action dated Mar. 12, 2015 in corresponding Chinese Patent Application No. 201280044329.7, along with an English translation of relevant portions thereof.
  • Decision on Grant dated Sep. 2, 2015 in corresponding Russian Patent Application No. 2014114490/02.
  • International Search Report dated Oct. 24, 2012 issued in corresponding International patent application No. PCT/EP2012/065219.
  • Korean Office Action dated Mar. 25, 2016 in corresponding Korean Patent Application No. 10-2014-7006182, along with an English translation of relevant portions thereof.