Patents
US 11,088,320 B2#61618164 Most CitedActiveUnited States (USPTO)Utility

Fabrication of large height top metal electrode for sub-60nm magnetoresistive random access memory (MRAM) devices

1Forward Citations (#61618164 Global)
0.2/yrCitation Velocity (#34420067 Global)
0.75Citation PageRank (#61618164 Global)
38Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process flow for forming magnetic tunnel junction (MTJ) cells with a critical dimension CD≤60 nm by using a top electrode (TE) hard mask having a thickness≥100 nm prior to MTJ etching is disclosed. A carbon hard mask (HM), silicon HM, and photoresist are sequentially formed on a MTJ stack of layers. A pattern of openings in the photoresist is transferred through the Si HM with a first reactive ion etch (RIE), and through the carbon HM with a second RIE. After TE material is deposited to fill the openings, a chemical mechanical process is performed to remove all layers above the carbon HM. The carbon HM is stripped and the resulting TE pillars are trimmed to a CD≤60 nm while maintaining a thickness proximate to 100 nm. Thereafter, an etch process forms MTJ cells while TE thickness is maintained at ≥70 nm.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 38 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method, comprising: forming a magnetic tunnel junction (MTJ) stack on a bottom electrode; forming a hard mask layer on the MTJ stack; forming an opening in the hard mask layer, the opening having a first dimension measured in a direction parallel to a top surface of the MTJ stack; filling the opening with a conductive material; after filling the opening, removing the hard mask layer to expose sidewalls of the conductive material; trimming the conductive material to form a top electrode (TE) pillar, the TE pillar having a second dimension, the second dimension being measured in the direction

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (38)

PatentTitleYearCitations
US 6,395,621 B1Method of manufacturing a semiconductor device with oxide mediated epitaxial layer200250
US 2003073251 A1Plate-through hard mask for MRAM devices—38
US 2003206434 A1Layout for thermally selected cross-point mram cell—36
US 6,806,096 B1Integration scheme for avoiding plasma damage in MRAM technology2004169
US 2005277207 A1Mask schemes for patterning magnetic tunnel junctions—28
US 6,984,529 B2Fabrication process for a magnetic tunnel junction device200669
US 7,001,783 B2Mask schemes for patterning magnetic tunnel junctions200657
US 7,060,194 B2Dry etching method for magnetic material200641
US 7,169,654 B2Method of forming a semiconductor device200717
US 2007215911 A1Magnetic tunnel junction patterning using Ta/TaN as hard mask—37
US 7,471,445 B2Fast-response micro-mechanical devices20089
US 2009078927 A1Composite hard mask for the etching of nanometer size magnetic multilayer based device—68
US 2009159563 A1Method for forming magnetic tunnel junction cell—38
US 7,593,193 B2Magnetoresistive element and magnetic memory device20098
US 2009261437 A1Two Mask MTJ Integration For STT MRAM—43
US 7,696,551 B2Composite hard mask for the etching of nanometer size magnetic multilayer based device201038
US 2010327248 A1Cell patterning with multiple hard masks—44
US 8,450,119 B2Magnetic tunnel junction patterning using Ta/TaN as hard mask201312
US 2013157383 A1Method for fabricating semiconductor device—4
US 8,716,072 B2Hybrid CMOS technology with nanowire devices and double gated planar devices20145
US 8,722,543 B2Composite hard mask with upper sacrificial dielectric layer for the patterning and etching of nanometer size MRAM devices201438
JP 2014130946 AMagnetoresistive element, magnetic storage device using the same, and manufacturing method of the same—13
US 2014235056 A1System, method and apparatus for ion milling in a plasma etch chamber—6
US 8,971,507 B2Facsimile server, facsimile system, and facsimile transmission method20151
US 9,142,761 B2Method for fabricating a magnetic tunnel junction device20153
US 9,166,154 B2MTJ stack and bottom electrode patterning process with ion beam etching using a single mask201540
US 9,269,894 B2Isolation of magnetic layers during etch in a magnetoresistive device201630
US 9,275,713 B2Magnetoresistive element and method of manufacturing the same201612
WO 2016/058008 A2Spin on hard-mask material—3