Porous monolith containing TiO2 and method for the production thereof
Abstract
The invention relates to a porous monolith comprising between 20 wt.-% and 70 wt.-% TiO 2 relative to the total weight of the monolith, and between 30 wt.-% and 80 wt.-% a refractory oxide, selected from silica, alumina or silica-alumina, relative to the total weight of the monolith, characterized in that said porous monolith has a bulk density of less than 0.19 g/mL.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A porous monolith comprising between 20% and 70% by weight of TiO 2 relative to the total weight of the monolith, between 30% and 80% by weight of a refractory oxide, which is silica, alumina or silica-alumina relative to the total weight of the monolith, and wherein said porous monolith has a bulk density of less than 0.19 g/ml.
- Claim 2Depends on #1
The monolith as claimed in claim 1 , having a bulk density of less than 0.16 g/ml.
- Claim 3Depends on #1
The monolith as claimed in claim 1 , which comprises a mesoporous volume of from 0.1 to 1 ml/g for a pore diameter between 0.2 and 50 nm.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (10)
Non-Patent Literature (2)
- English Abstract of JP 2009-007219 A published Jan. 15, 2009.
- International Search Report dated Jun. 19, 2018 issued in corresponding PCT/EP2018/060376 application (3 pages).