Glass substrate for display and method for producing same
Abstract
Provided are: a glass substrate that achieves a high strain point while having a low devitrification temperature; and a method for producing said glass substrate. This glass substrate for a display is made of a glass comprising SiO2 and Al2O3, comprising 0% or more to less than 3% B2O3 and from 5 to 14% BaO in mass %, and substantially devoiding Sb2O3, wherein the devitrification temperature is 1235° C. or lower and the strain point is 720° C. or higher. Alternatively, this glass substrate for a display is made of a glass comprising SiO2 and Al2O3, comprising 0% or more to less than 3% B2O3, 1.8% or more MgO, and from 5 to 14% BaO in mass %, and substantially devoiding Sb2O3, wherein (SiO2+MgO+CaO)—(Al2O3+SrO+BaO) is less than 42%, the devitrification temperature is 1260° C. or lower, and the strain point is 720° C. or higher. This method for producing said glass substrate for a display comprises: a melting step for melting, by using at least direct electrical heating, a glass material prepared to have a predetermined composition; a forming step for forming, into a flat glass sheet, the molten glass that has been melted in the melting step; and an annealing step for annealing the f
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 33 · Forward citations: 0.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A glass substrate for a display composed of a glass, the glass comprising SiO 2 and Al 2 O 3 , wherein the Al 2 O 3 content is in a range of 16 to 35% by mass; and the glass further comprising, in % by mass, B 2 O 3 at greater than 0% and less than 3%; and Li 2 O in the range of 0 to 0.5%, and Na 2 O in the range of 0 to 0.5%, and K 2 O in the range of 0.1 to 0.8%, and wherein a mass ratio (B 2 O 3 /RO) is in the range of 0.03 to 0.5, the mass ratio (MgO/(RO+ZnO)) is in the range of 0.17 to 0.8, RO represents MgO+CaO+SrO+BaO, and the glass is devoid of Sb 2 O 3 , ZrO 2 , and TiO 2 , has a d
- Claim 2Depends on #1
The glass substrate according to claim 1 , wherein the glass substrate has a heat shrinkage rate of 15 ppm or
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (33)
Non-Patent Literature (5)
- Communication dated Apr. 16, 2021, from the State Intellectual Property Office of the P.R. of China in Application No. 201680037857.8.
- Communication dated Dec. 18, 2020 from the Korean Intellectual Property Office issued in corresponding Korean Application No. 10-2018-7002478.
- Communication dated Feb. 21, 2020 from the Intellectual Property of India in application No. 201847002506.
- Communication dated Jan. 25, 2021 from the Indian Patent Office issued in corresponding Indian Application No. 201847002506.
- Communication dated Jan. 7, 2020 from Japanese Patent Office in JP Application No. 2017-526371.