Patents
US 11,053,576 B2#44126414 Most CitedActiveUnited States (USPTO)Utility

Method for producing aluminum alloy rolled material for molding having excellent bending workability and ridging resistance

2Forward Citations (#44126414 Global)
0.4/yrCitation Velocity (#20589380 Global)
0.91Citation PageRank (#46941650 Global)
35Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present disclosure relates to a method for producing an aluminum alloy rolled material for deformation molding, the method including: a step of performing homogenization treatment of an ingot including an aluminum alloy with predetermined composition; a step of cooling the aluminum alloy after the homogenization treatment so that an average cooling rate in an ingot thickness of ¼ part from 500° C. to 320° C. is 30° C./h to 2000° C./h; and a step of starting hot rolling at 370° C. to 440° C. and winding the hot-rolled aluminum alloy at 310 to 380° C., in which the method for producing an aluminum alloy rolled material for deformation molding further includes a step of retaining the aluminum alloy after the cooling step for 0.17 hours or more at a heating temperature before rolling set within a range of 370° C. to 440° C. before the hot rolling.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 35 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing an aluminum alloy rolled material for deformation molding, the method comprising: a step of performing homogenization treatment of an ingot comprising an aluminum alloy comprising Si: 0.30 to 1.50 mass %, Mg: 0.30 to 1.50 mass %, Cu: 0.001 to 1.50 mass %, at least any of 0.50 mass % or less of Mn, 0.40 mass % or less of Cr, and 0.40 mass % or less of Fe, and a balance of Al and inevitable impurities; a cooling step of cooling the aluminum alloy after the homogenization treatment in a single cooling process from a temperature at the homogenization treatment to an end temp

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (35)

PatentTitleYearCitations
JP S59685 AWorld timepiece—7
JP H07228956 AProduction of aluminum alloy sheet for forming work—37
JP 2,823,797 B2成形加工用アルミニウム合金板の製造方法199810
JP 2001342577 AAluminum alloy plate superior in press formability—12
US 2002005232 A1Aluminum alloy plate excelling in filiform corrosion resistance and method of fabricating same—12
JP 2002146462 AAluminum alloy sheet having excellent formability and its production method—12
JP 2003226926 AAluminum alloy sheet having excellent bending workability and production method thereof—23
JP 2003277870 AAluminum alloy sheet having excellent bending workability and hardenability in coating/baking, and production method thereof—10
JP 2004010982 AAluminum alloy sheet having excellent bending workability and press formability—15
JP 2004124213 AAluminum alloy sheet for panel forming, and its manufacturing method—14
US 2004094249 A1Aluminum alloy sheet excellent in formability and hardenability during baking of coating and method for production thereof—37
JP 3,590,685 B2自動車外板用アルミニウム合金板の製造方法20043
JP 2006241548 AAl-Mg-Si ALLOY SHEET SUPERIOR IN BENDABILITY, MANUFACTURING METHOD THEREFOR, AND AUTOMOTIVE SKIN PLATE OBTAINED FROM THE SHEET—14
US 2007209739 A1Method for producing Al-Mg-Si alloy sheet excellent in bake-hardenability and hemmability—23
JP 2008045192 AAluminum alloy sheet showing excellent ridging-mark resistance at molding—24
US 2008175747 A1Aluminum alloy sheet—24
US 2009081072 A1Aluminum alloy sheet and method for manufacturing the same—8
KR 20090104739 AAlluminum alloy sheet superior in paint baking hardenability and invulnerable to room temperature aging, and method for production thereof—5
WO 2009/123011 A1Aluminum alloy sheet with excellent post-fabrication surface qualities and method of manufacturing same—5
JP 2009263781 AAluminum alloy sheet with excellent post-fabrication surface quality and method of manufacturing same—21
JP 2010242215 AAluminum alloy sheet having excellent ridging mark property upon forming—30
US 2011017370 A1Aluminum alloy sheet with excellent post-fabrication surface qualities and method of manufacturing same—10
JP 2012077319 AAluminum alloy sheet for forming excellent in bending workability and method for producing the same—8
JP 2012077318 AAluminum alloy rolled sheet for molding process having excellent ridging resistance and method for producing the same—14
JP 2012214846 AAluminum alloy sheet for molding process and method for producing the same—17
US 2012291924 A1Aluminum alloy sheet and method for manufacturing the same—4
US 2013164170 A1Aluminum alloy material for storage container for high-pressure hydrogen gas—12
US 2014166162 A1Aluminum alloy sheet and method for manufacturing same—10

Non-Patent Literature (5)

  • English Translation of JP 2008-045192, JPlatPat (Year: 2020).
  • English Translation of JP 2010-242215 A, Espacenet (Year: 2019).
  • Japanese office action issued in Japanese Patent App. No. 2017-025445, dated Apr. 18, 2017 (with translation).
  • Korean office action issued by KIPO dated Mar. 20, 2018 (with translation).
  • Written opinion of the Int'l. Searching Authority issued in Int'l. App. No. PCT/JP2017/025401, dated Nov. 13, 2017.