Patents
US 11,024,501 B2#22282102 Most CitedActiveUnited States (USPTO)Utility

Carrier-assisted method for parting crystalline material along laser damage region

5Forward Citations (#22282102 Global)
1.0/yrCitation Velocity (#7104114 Global)
1.20Citation PageRank (#32403171 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for removing a portion of a crystalline material (e.g., SiC) substrate includes joining a surface of the substrate to a rigid carrier (e.g., >800 μm thick), with a subsurface laser damage region provided within the substrate at a depth relative to the surface. Adhesive material having a glass transition temperature above 25° C. may bond the substrate to the carrier. The crystalline material is fractured along the subsurface laser damage region to produce a bonded assembly including the carrier and a portion of the crystalline material. Fracturing of the crystalline material may be promoted by (i) application of a mechanical force proximate to at least one carrier edge to impart a bending moment in the carrier; (ii) cooling the carrier when the carrier has a greater coefficient of thermal expansion than the crystalline material; and/or (iii) applying ultrasonic energy to the crystalline material.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 5.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A crystalline material processing method comprising: temporarily bonding a rigid carrier having a thickness of greater than 800 microns to a first surface of a crystalline material comprising a semiconductor with an intervening adhesive material, wherein the crystalline material comprises a substrate having a subsurface laser damage region at a depth relative to the first surface, the rigid carrier has a modulus of elasticity of at least 20 GPa, and the adhesive material has a glass transition temperature T g of greater than 25° C.; and fracturing the crystalline material along or proximate t

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗