Patents
US 10,995,403 B2#45381855 Most CitedActiveUnited States (USPTO)Utility

Method of forming aluminum nitride film and method of manufacturing semiconductor light-emitting element

2Forward Citations (#45381855 Global)
0.4/yrCitation Velocity (#20706772 Global)
0.86Citation PageRank (#49966113 Global)
42Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of forming an aluminum nitride film includes: preparing a substrate that comprises, in a surface thereof, a plurality of concave portions that are separated from each other; forming an aluminum nitride film on said surface of the substrate and on an inner surface of each of the concave portions such that open holes are formed in a portion of the aluminum nitride film corresponding to each of the concave portions, each of the holes being smaller than each of openings of the concave portions; and applying heat treatment to the substrate with the aluminum nitride film formed thereon in a nitrogen gas containing a carbon monoxide gas to close the holes formed in the aluminum nitride film.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 42 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of forming an aluminum nitride film, the method comprising: preparing a substrate that comprises, in a surface thereof, a plurality of concave portions that are separated from each other, wherein each of the concave portions has an opening; forming an aluminum nitride film on said surface of the substrate and on an inner surface of each of the concave portions such that open holes are formed in a portion of the aluminum nitride film corresponding to the concave portions, wherein each of the open holes has an opening and corresponds to a respective one of the concave portions, and wher

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (42)

PatentTitleYearCitations
US 6,153,010 AMethod of growing nitride semiconductors, nitride semiconductor substrate and nitride semiconductor device2000695
US 6,503,610 B2Group III-V compound semiconductor and method of producing the same200345
US 2003203531 A1Defect-free semiconductor templates for epitaxial growth and method of making same—38
JP 2004111766 AGallium nitride-based semiconductor device and its manufacturing method—56
US 2005287774 A1Method of improving surface flatness of group-III nitride crystal, substrate for epitaxial growth, and semiconductor device—19
US 7,141,444 B2Production method of III nitride compound semiconductor and III nitride compound semiconductor element200625
JP 2006332570 AMethod for improving surface flatness of group iii nitride crystal, substrate for epitaxial growth and semiconductor device—18
JP 2008060519 AMETHOD OF DECREASING DISLOCATIONS IN EPITAXIAL FILM OF AlN-BASED GROUP III NITRIDE—29
JP 2008115023 AMETHOD FOR MANUFACTURING AlN-BASED GROUP III NITRIDE SINGLE CRYSTAL THICK FILM—20
US 2009166650 A1Light-emitting device of group iii nitride-based semiconductor and manufacturing method thereof—13
JP 2009242130 ASubstrate for epitaxial growth and method for manufacturing the same, and group iii nitride semiconductor element—27
US 2010032647 A1Utlraviolet light emitting devices and methods of fabrication—62
US 2010065854 A1Growth and manufacture of reduced dislocation density and free-standing aluminum nitride films by hydride vapor phase epitaxy—24
US 7,687,824 B2Method of improving surface flatness of group-III nitride crystal, substrate for epitaxial growth, and semiconductor device20108
US 2010099213 A1Method for blocking dislocation propagation of semiconductor—11
US 2011163295 A1Semiconductor with low dislocation—14
US 2012258286 A1Template for Epitaxial Growth and Process for Producing Same—18
US 2013056770 A1Patterned Substrate Design for Layer Growth—23
US 2014134773 A1Patterned Layer Design for Group III Nitride Layer Growth—38
JP 2015042598 ASubstrate having aluminum nitride (ain) film and method for manufacturing aluminum nitride (ain) film—21
US 9,000,415 B2Light emitting device20152
US 9,048,347 B2Epitaxial structure including carbon nanotube layer in grooves20154
US 2015340558 A1Light emitting diode chip—22
US 2015372190 A1Ultraviolet light emitting diode and method for producing same—24
US 9,318,326 B2Dislocation and stress management by mask-less processes using substrate patterning and methods for device fabrication20168
US 2016190387 A1Strain-Control Heterostructure Growth—11
US 2016254411 A1Substrate having annealed aluminum nitride layer formed thereon and method for manufacturing the same—28
US 2016265138 A1Template for Epitaxial Growth, Method for Producing the Same, and Nitride Semiconductor Device—3

Non-Patent Literature (5)

  • Fukuyama et al., Single crystalline aluminum nitride films fabricated by nitriding α-Al2O3, Jul. 20, 2006, J. Applied Physics, vol. 100, No. 024905, pp. 024905-1 to 024905-7. (Year: 2006).
  • H. Fukuyama et al., Nitridation behavior of sapphire using a carbon-saturated N2—CO gas mixture, Feb. 16, 2010, J. Applied Physics, vol. 107, No. 043502, pp. 043502-1 to 043502-7. (Year: 2010).
  • H. Miyake et al., Annealing of an AIN buffer layer in N2—CO for growth of a high quality AIN film on sapphire, Jan. 6, 2016, Applied Physics Express, vol. 9, No. 025501, pp. 1-4. (Year: 2016).
  • K. Fujita et al., HVPE growth of thick AIN on trench-patterned substrate, Mar. 23, 2011, Physica Status Solidi C, vol. 8, No. 5, pp. 1483-1486. (Year: 2011).
  • Machine translation, Noguchi, WO 2017/134708, translation date: Jul. 31, 2020, Espacenet, all pages (Year: 2020).