Abstract

The present invention relates to a method for producing an impregnated pitch from a petroleum-based raw material and to an impregnated pitch produced using the same, and when the method for producing an impregnated pitch according to the present invention is used, it is possible to produce an impregnated pitch having a high carbonization yield (40 wt % or more) and low quinoline insoluble matter (QI, 2% or less) for improving efficiency of an impregnation process from a petroleum-based raw material. Therefore, when an impregnation process is applied to a carbon compact by using the impregnated pitch according to the present invention, it is possible to remarkably reduce micropores inside the carbon compact, and to produce a carbon compact having physical properties such as excellent electrical conductivity and mechanical strength.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for producing an impregnated pitch comprising the following steps: heat-treating a petroleum-based raw material in an inert gas atmosphere under the pressure of 10˜40 bar (step 1); heat-treating the petroleum-based raw material which had been heat-treated in step 1 at normal pressure (step 2); and distillating the petroleum-based raw material which had been heat-treated in step 2 under reduced pressure (step 3).

  2. Claim 2Depends on #1

    The method for producing an impregnated pitch according to claim 1 , wherein the heat-treatment in step 1 is performed in a temperature range of 300° C. to 450° C.

  3. Claim 3Depends on #1

    The method for producing an impregnated pitch according to claim 1 , wherein the heat-treatment in step 1 is performed for 0.5˜10 hours.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (1)

  • English Translation of PCT International Search Report dated Mar. 30, 2018, from which the instant application is based, 2 pgs.