Patents
US 10,828,702 B2#99656552 Most CitedActiveUnited States (USPTO)Utility

Silver powder and method for producing same

0Forward Citations (#99656552 Global)
0.0/yrCitation Velocity (#99656552 Global)
0.56Citation PageRank (#99656552 Global)
19Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

There is provided a silver powder which has a small average particle diameter and a small thermal shrinkage percentage, and a method for producing the same. While a molten metal of silver heated to a temperature (1292 to 1692° C.), which is higher than the melting point (962° C.) of silver by 330 to 730° C., is allowed to drop, a high-pressure water is sprayed onto the molten metal of silver (preferably at a water pressure of 90 to 160 MPa) to rapidly cool and solidify the molten metal of silver to powderize silver to produce a silver powder which has an average particle diameter of 1 to 6 μm and a shrinkage percentage of not greater than 8% (preferably not greater than 7%) at 500° C., the product of the average particle diameter by the shrinkage percentage at 500° C. being 1 to 11 μm·% (preferably 1.5 to 10.5 μm·%).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for producing a silver powder consisting of silver, said method comprising the steps of: preparing a molten metal of silver heated to a temperature which is higher than a melting point of silver by 438 to 730° C.; and powderizing silver by rapidly cooling and solidifying the molten metal by spraying a high-pressure water onto the molten metal while the molten metal is allowed to drop.

  2. Claim 2Depends on #1

    A method for producing a silver powder as set forth in claim 1 , wherein said high-pressure water is sprayed onto the molten metal at a water pressure of 90 to 160 MPa.

  3. Claim 3Depends on #1

    A method for producing a silver powder as set forth in claim 1 , wherein said silver powder has an average particle diameter of 1 to 6 μm.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (19)

Non-Patent Literature (3)

  • Ankus et al., "The water atomization of silver: effect of pressure and superheat" Powder Technology, 73 (1992), pp. 169-179.
  • International search report for patent application No. PCT/JP2016/004706 dated Jan. 20, 2017.
  • Supplementary European search report for patent application No. 16 85 9295 dated Apr. 3, 2019.