Provided is a high-light transmittance zirconia sintered body, prepared by processing and forming a material for the high-light transmittance zirconia sintered body, and then performing high-temperature sintering in the atmosphere under normal pressure. The material for a high-light transmittance zirconia sintered body is prepared from zirconia powder and α-aluminum oxide as raw materials, wherein the molar percentage of yttrium oxide in the zirconia powder is 4-6%. The high-light transmittance zirconia sintered body can be used for preparing a fixed dental prosthesis. The zirconia sintered body has a grain size of 0.1-0.7 μm, and due to the dispersion and toughening by aluminum oxide, the zirconia sintered body has a higher strength and toughness. Pores in the zirconia powder can be eliminated by adding aluminum oxide. The zirconia sintered body has a higher light transmittance, and the prepared dentures are good in texture, good in jade-like appearance, and closer to the human teeth.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for preparing a material for a high-light transmittance zirconia sintered body, comprising: adding an appropriate amount of water to zirconia powder and grinding, during which α-aluminum oxide powder is added, then spray granulating to obtain a powder material having an average particle diameter of 0.1 μm to 0.4 μm; wherein the molar percentage of yttrium oxide in the zirconia powder is 4% to 6%.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the zirconia powder has a BET specific surface area of 8 to 16 m 2 /g, and an average particle diameter of 0.1 to 0.4 μm; and wherein the method further comprises preparing the zirconia powder comprising: mixing a soluble zirconium salt and a soluble yttrium salt at a ratio and dissolving in water to form a slurry, and wherein pH of the slurry is adjusted to 8 to 10 with ammonia water whil

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (14)