Sterling silver alloy and articles made from the same
Abstract
An improved sterling silver alloy. Like all sterlings, the improved alloy is at least 92.5 percent silver by weight. It has less copper than traditional sterlings: 3.0 percent versus the traditional 7.5 percent. Additionally, the improved alloy includes about 2.75 percent palladium, about 1.0 percent tin, and about 0.75 percent zinc, all by weight. A grain refiner, such as ruthenium, may also be provided. The components of the preferred alloy are melted, degassed, remelted, and then formed into casting grains, wire, and etc. The resulting alloy is significantly harder, as cast, than traditional sterlings: 95-120 Vickers versus 65 Vickers for traditional sterlings. The improved alloy also exhibits improved corrosion resistance. Other than a slightly higher (<200° F.) liquidus temperature, the improved alloy may be worked in substantially the same manner as traditional sterlings. Pieces cast from the improved alloy may be age hardened to about 160 Vickers, if desired.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of making one or more jewelry articles comprising: placing a casting grains of an alloy in a crucible, wherein said alloy comprises at least 92.5 percent, by weight, silver; about 3.0 percent, by weight, copper; about 2.75 percent, by weight, palladium; about 1.0 percent, by weight, tin; and completely melting said casting grains by heating said crucible to a temperature of at least about 1790 degrees F.; pouring said molten alloy into an investment mold containing one or more jewelry article shaped cavities; allowing said molten alloy to cool and solidify within said investment mold
- Claim 2Independent Claim
A method of making one or more jewelry
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 12,180,574 B1 | Tarnish resistant and age hardenable sterling silver alloy | 2024 | 0 |
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- Davis, et al, "Precious Metals and Alloys", Metals Handbook Desk Edition, 1998, ASM International, p. 1-25.
- McDonald, A.S. & Sistare, G.H.; The Metallurgy of Some Carat Gold Jewellery Alloys; Gold Bulletin (1978); p. 69.
- Michael T. Roche and Frank E. Goodwin, Improved Tarnish Resistant Sterling Silver, Sep. 2003, Research Consortium, Durham, NC, USA.
- Pitwonka, Thomas S., "Molding Methods-Investment Casting", 1998, Metals Handbook, 2nd Edition, ASM International, p. 1-13.
- Pitwonka, Thomas S., “Molding Methods—Investment Casting”, 1998, Metals Handbook, 2nd Edition, ASM International, p. 1-13.