Methods and systems for suppressing corrosion of metal surfaces

1Forward Citations (#62037763 Global)
0.2/yrCitation Velocity (#37784316 Global)
0.74Citation PageRank (#62037763 Global)
46Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Certain metal surfaces are often unable to be effectively contacted with fluids containing hydrofluoric acid due to significant corrosion issues. Titanium and titanium alloy surfaces represent but one example. Corrosion inhibitor compositions comprising an N-(phosphonoalkyl)iminodiacetic acid or any salt thereof can be used to suppress metal corrosion, including that taking place on titanium and titanium alloy surfaces. Methods for suppressing corrosion of a metal surface can comprise: contacting a metal surface with a corrosive environment, the corrosive environment comprising hydrofluoric acid; introducing a corrosion inhibitor composition to the corrosive environment, the corrosion inhibitor composition comprising an N-(phosphonoalkyl)iminodiacetic acid or any salt thereof; contacting the metal surface with the corrosion inhibitor composition; and allowing the corrosion inhibitor composition to suppress corrosion of the metal surface being contacted by the corrosive environment.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 46 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method comprising: contacting a metal surface with a corrosive environment, the corrosive environment comprising hydrofluoric acid; introducing a corrosion inhibitor composition to the corrosive environment, the corrosion inhibitor composition comprising an N-(phosphonoalkyl)iminodiacetic acid or any salt of the N-(phosphonoalkyl)iminodiacetic acid, wherein the N-(phosphonoalkyl)iminodiacetic acid is initially fully protonated; contacting the metal surface with the corrosion inhibitor composition; and suppressing corrosion of the metal surface being contacted by the corrosive environment thr

  2. Claim 2Depends on #1

    The method of claim 1 , wherein a hydrofluoric acid concentration in the corrosive environment ranges between 0.25 M and 5 M.

  3. Claim 3Depends on #2

    The method of claim 2 , w

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (46)

PatentTitleYearCitations
US 3,222,289 ADissolution of zirconium in titanium equipment19659
US 5,019,343 AControl of corrosion in aqueous systems using certain phosphonomethyl amines199163
US 5,051,197 AScale removal treatment199116
US 5,120,471 AProcess and composition for protecting chrome steel199266
US 5,171,460 AMethod for preventing metal carbonate scale formation in a well penetrating a subterranean formation199219
EP 0,534,621 A1Method of inhibiting corrosion in acidizing wells—4
US 5,294,371 ACorrosion and/or scale inhibition199456
US 5,529,125 AAcid treatment method for siliceous formations1996106
US 5,543,388 AIntensified corrosion inhibitor and method of use199633
US 6,001,186 AAcid cleaning/deoxidizing aluminum and titanium without substantial etching19999
US 6,117,364 AAcid corrosion inhibitor2000106
US 6,506,711 B1Reducing aluminum compound precipitation during subterranean formation acidizing200335
US 2004254079 A1Composition and Method for Treating a Subterranean Formation—64
GB 2,404,211 ABuffered hydrofluoric acidizing process—4
US 2005016731 A1Acidizing stimulation method using a pH buffered acid solution—33
EP 1,163,969 B1High strength pipe of an alpha plus beta titanium alloy and method for its manufacture.20054
US 2006054325 A1Solid sandstone dissolver—22
US 2006131022 A1Matrix treatment of damaged sandstone formations using buffered HF-acidizing solutions—34
US 2006219661 A1Surface treatment methods for implants made of titanium or titanium alloy—28
US 2006281636 A1Single fluid acidizing treatment—18
US 7,192,908 B2Composition and method for treating a subterranean formation200748
US 2007071887 A1Methods of inhibiting corrosion of a metal surface—30
US 2007235189 A1Method for Treating a Subterranean Formation—69
US 2008006409 A1Solid Sandstone Dissolver—13
WO 2008/077005 A1Corrosion inhibitor composition comprising a built-in intensifier—7
US 2008200354 A1Breaker and displacement fluid and method of use—83
US 2008280046 A1Process for treating metal surfaces—34
US 2009042748 A1Method of Acidizing Sandstone Formations—58
GB 2,453,630 AAqueous well treatment fluid containing fluoride, boron and phosphonate—6

Non-Patent Literature (5)

  • "Corrosion Resistant Alloys for Deep Offshore Drilling by High Density Infrared Fusion Process", T1S402 Paper. Retrieved from URL: http://pennwell.sds06.websds.net/2013/dot/papers/T1S402-paper.pdf on Apr. 12, 2017 (19 pages).
  • Aboud, Ricardo Salomao et al. "Effective Matrix Acidizing in High-Temperature Environments." SPE Annual Technical Conference and Exhibition, Society of Petroleum Engineers, 2007.
  • Baxter, Carl F. et al. "Experience and Guidance in the Use of Titanium Components in Steel Catenary Riser Systems." OTC 18624, In Offshore Technology Conference, Offshore Technology Conference, Apr. 30-May 3, 2007 (13 pages).
  • Denney, Dennis. "Ultradeep HP/HT Completions: Classification, Design Methodologies, and Technical Challenges", J. Petroleum Technologies, pp. 83-85, Mar. 2007.
  • G. Mohammed, and A. Galadima. The Chemistry Scale Inhibitors and the Mechanism of Interactions with Carbonate Reservoir Rock. (Year: 2011).