Method for increasing the particle size of ammonium octamolybdate (AOM)
Abstract
Methods of increasing the particle size of ammonium octamolybdate (AOM) pigment powder are provided. A method can include heating the AOM pigment powder to a temperature above 20° C. for a given amount of time. An ink composition can be produced by formulating AOM pigment powder with increased particle size and incorporating the AOM pigment powder into an ink composition.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of increasing the particle size of ammonium octamolybdate (AOM) pigment powder, the method comprising the following steps performed in order: (a) storing the AOM pigment powder in a sealed container at a temperature (k2) below 10° C. for at least 4 hours; (b) exposing the AOM pigment powder to air at the temperature (k2) for at least 4 hours; and (c) heating the AOM pigment powder in a sealed container to a temperature (k1) above 30° C. for at least 4 hours.
- Claim 2Depends on #1
The method according to claim 1 wherein the air has a relative humidity in the range of 40 to 100%.
- Claim 3Depends on #1
The method according to claim 1 , which results in AOM having a D10 particle size of more than 0.4 microns.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (13)
Non-Patent Literature (1)
- International Search Report/Written Opinion, International Application No. PCT/GB2015/053574, PCT/ISA/210, PCT/ISA/237, dated Jan. 29, 2016.