Low contrast anti-reflection articles with reduced scratch and fingerprint visibility
Abstract
Embodiments of articles including a low-contrast anti-reflection coating are disclosed. The coated surface of such articles exhibits a reduced difference in reflectance between a pristine state and when a surface defect is present. In one or more embodiments, the coated surface of such articles exhibits a first average reflectance in the range from about 0.6% to about 6.0% in a pristine condition and a second average reflectance of about 8% or less after removal of a surface thickness of the anti-reflection coating. In other embodiments, the coated substrate exhibits a second average reflectance of about 10% or less, when the coated surface comprises a contaminant. In some embodiments, the coated substrate exhibits a first color coordinate (a*1, b*1) in a pristine condition and a second color coordinate (a*2, b*2) after the presence of a surface defect such that Δa*b* is about 6 or less.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 27 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An article comprising: a substrate having a substrate surface; and an anti-reflection coating disposed on the substrate surface forming a coated surface, wherein the anti-reflection coating comprises a first low RI sub-layer and a second high RI sub-layer, wherein the first low RI sub-layer comprises SiO 2 , wherein the second high RI sub-layer comprises Si u Al v O x N y , AlO x N y , or combinations thereof, wherein the coated surface exhibits a first average reflectance when the coated surface is in a pristine condition, and a second average reflectance after removal of a surface thickness
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 12,422,604 B2 | Hardened optical windows for LIDAR applications at 850-950NM | 2025 | 0 |
References Cited — Backward Prior Art (27)
Non-Patent Literature (5)
- English Translation of CN201580039267.4 Office Action dated Jan. 22, 2018; 9 pages; Chinese Patent Office.
- English Translation of JP2016568004 Office Action dated Mar. 6, 2019, Japan Patent Office, 6 Pgs.
- English Translation of TW104116507 Search Report dated Mar. 14, 2019, Taiwan Patent Office, 1 Pg.
- International Search Report and Written Opinion of the International Searching Authority; PCT/US2015/032138; dated Oct. 28, 2015.
- Oliver, W.C.; Pharr, G. M. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. J. Mater. Res., vol. 7, No. 6, 1992, 1564-1583.