Austenitic alloy
Abstract
An austenitic alloy comprising (in weight %): C: 0.01-0.05 Si: 0.05-0.80 Mn: 1.5-2 Cr: 26-34.5 Ni: 30-35 Mo: 3-4 Cu: 0.5-1.5 N: 0.05-0.15 V: ≤0.15 the balance being Fe and unavoidable impurities, characterized in that 40≤% Ni+100*% N≤50.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
An austenitic alloy comprising in weight %: C: 0.01-0.015 Si: 0.40-0.52 Mn: 1.7 Cr: 27 Ni: 33 Mo: 3.4 Cu: 0.9-1.0 N: 0.09-0.11 V: 0.07-0.09 the balance being Fe and unavoidable impurities, wherein the weight % of N and Ni is balanced to fulfill the requirement 40<% Ni+100*% N<50, and wherein the alloy has a microstructure that includes a MX phase.
- Claim 2Depends on #1
The austenitic alloy according to claim 1 , wherein the weight % of N and Ni is balanced to fulfill the requirement 40<% Ni+100*% N<45.
- Claim 3Depends on #1
The austenitic alloy according to claim 1 , wherein a creep test at 600° C. and a stress of 160 MPa exhibits a rupture elongation of 71 to 90% and a time to rupture of at least 100,000 hours, and wherein a creep test at 650° C. and a stress of 95 to 105 MPa exhibits a rupture elongatio
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (22)
Non-Patent Literature (2)
- J. Keiser et al. "Recovery Boiler Superheater Corrosion Field Study", Oak Ridge National Laboratory, NACE Corrosion 2010, Paper No. 10081, pp. 1-18 (2010).
- Notice of Reasons for Rejection for Japanese Application No. 2014-552606 dated Sep. 20, 2016.