Patents
US 10,456,751 B2#61178309 Most CitedActiveUnited States (USPTO)Utility

Method for producing hollow fiber carbon membrane and separation membrane module

1Forward Citations (#61178309 Global)
0.1/yrCitation Velocity (#40723711 Global)
0.75Citation PageRank (#61178309 Global)
9Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

An object of the present invention is to provide a method capable of easily controlling the permeation rate and the selectivity of gas molecules, in a hollow fiber carbon membrane which can be used as a gas separation membrane. The present invention provides a method of producing a hollow fiber carbon membrane, the method including: a preparation step of preparing a precursor made of an organic polymer compound in the form of a hollow fiber; a preheating step of heating the precursor to a temperature of 150° C. to 400° C. in an atmosphere containing an oxygen gas; and a carbonization step of heating the precursor which has been subjected to the preheating step to a temperature of 450° C. to 850° C., thereby carbonizing the precursor; wherein the carbonization step includes heating the precursor in the presence of a hydrocarbon gas which may contain a nitrogen atom and which has from 1 to 8 carbon atoms. This method allows for easily controlling the permeation rate and the selectivity of gas molecules, in the resulting hollow fiber carbon membrane.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 1.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of producing a hollow fiber carbon membrane, the method comprising: a preparation step of preparing a precursor made of an organic polymer compound in the form of a hollow fiber; a preheating step of heating the precursor to a temperature of 150° C. to 400° C. in an atmosphere containing an oxygen gas; and a carbonization step of heating the precursor which has been subjected to the preheating step to a temperature of 450° C. to 850° C., thereby carbonizing the precursor; wherein the carbonization step comprises heating the precursor in the presence of a hydrocarbon gas which may cont

  2. Claim 2Depends on #1

    The method of producing a hollow fiber carbon membrane according to claim 1 , wherein the hydrocarbon g

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

Non-Patent Literature (4)

  • English language machine translation of JP 2002-235538. Retrieved from https://worldwide.espacenet.com on May 20, 2019. (Year: 2019).
  • Geiszler, Vincent C. et al., "Effects of Polyimide Pyrolysis Conditions on Carbon Molecular Sieve Membrane Properties", Ind. Eng. Chem. Res., 1986, 35, pp. 2999-3003. (Year: 1986).
  • International Preliminary Report on Patentability in International Application No. PCT/JP2016/056497 dated Oct. 12, 2017, 8 pages.
  • International Search Report, corresponding International Application No. PCT/JP2016/056497, dated Apr. 19, 2016.