Patents
US 10,446,286 B2#61400448 Most CitedActiveUnited States (USPTO)Utility

Method for vitrification of waste

1Forward Citations (#61400448 Global)
0.1/yrCitation Velocity (#40739697 Global)
0.75Citation PageRank (#61400448 Global)
5Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for vitrifying waste to prevent the formation of molybdate secondary phases includes forming a feed mixture that includes the waste, a source of vanadium, and at least one of glass frit or glass forming chemicals and vitrifying the feed mixture in a melter to produce a glass product that includes the waste.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for vitrifying waste comprising: forming a feed mixture that includes the waste, a source of vanadium oxide, and at least one of glass frit or glass forming chemicals; and vitrifying the feed mixture in a melter to produce a glass product that includes the waste.

  2. Claim 2Depends on #1

    The method of claim 1 wherein the glass product includes no more than 10 wt % vanadium oxide.

  3. Claim 3Depends on #1

    The method of claim 1 wherein the source of vanadium oxide is an additive that is combined with the waste.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗