Abstract

A semiconductor structure having a multiple-porous graphene layer includes a sapphire substrate, a single or multiple layer porous graphene film, and a gallium nitride layer. A fabrication method for forming the semiconductor structure having a single or multiple layer porous graphene film, includes: firstly, growing up the graphene on the copper foil; then, using the acetone and isopropyl alcohol to wash the sapphire substrate, and then using the nitrogen flow to dry up; transferring the graphene onto the semiconductor substrate, using the Poly(methyl methacrylate) to fix the single or multiple layer porous graphene film, and using the acetone to wash up; using the photolithography process to etch the whole surface of the multiple-porous graphene layer; and, using the metalorganic chemical vapor deposition to deposit gallium nitride on the single or multiple layer porous graphene film and the sapphire substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A semiconductor structure having a single-layer porous graphene film with a thickness of about 0.34 nm, formed by a low pressure chemical vapor deposition (LPCVD) and a metalorganic chemical vapor deposition (MOCVD), comprising: a sapphire substrate; wherein said single-layer porous graphene film having the thickness of about 0.34 nm is provided on said sapphire substrate, said single-layer porous graphene film being formed on a metal foil by the low pressure chemical vapor deposition (LPCVD) at 900° C. to 1100° C. via passing through methane (CH 4 ) and hydrogen (H 2 ), wherein said metal foi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

Non-Patent Literature (5)

  • Bai, Graphene nanomesh, Nature nanotechnology, vol. 5, Mar. 2010, pp. 190-194.
  • Kobayashi et al. Production of a 100-m-long high-quality graphene transparent conductive film by roll-to-roll chemical vapor deposition and transfer process. Applied Physics Letters, 102, pp. 023112 (2013).
  • Ni, Graphene Thickness Determination Using Reflection and Contrast Spectroscopy, Nano Letters, 2007, vol. 7, No. 0, pp. 2758-2763.
  • Russo et al. Synthesis, Properties and Potential Applications of Porous Graphene: A Review. Nano-Micro Lett. 594), 260-273 (2013_, pp. 260-273.
  • Sze, Semiconductor Devices. Physics and Technology, ed. 2, 2002, p. 292.