Patents
US 10,367,188 B2#59717888 Most CitedActiveUnited States (USPTO)Utility

Storage battery electrode, manufacturing method thereof, storage battery, and electronic device

1Forward Citations (#59717888 Global)
0.1/yrCitation Velocity (#40612681 Global)
0.77Citation PageRank (#59717888 Global)
50Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

In manufacturing a storage battery electrode, a method for manufacturing a storage battery electrode with high capacity and stability is provided. As a method for preventing a mixture for forming an active material layer from becoming strongly basic, a first aqueous solution is formed by mixing an active material exhibiting basicity with an aqueous solution exhibiting acidity and including an oxidized derivative of a first conductive additive; a first mixture is formed by reducing the oxidized derivative of the first conductive additive by drying the first aqueous solution; a second mixture is formed by mixing a second conductive additive and a binder; a third mixture is formed by mixing the first mixture and the second mixture; and a current collector is coated with the third mixture. The strong basicity of the mixture for forming an active material layer is lowered; thus, the binder can be prevented from becoming gelled.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a storage battery electrode, comprising: forming a first aqueous solution by mixing an active material with an aqueous solution including an oxidized derivative of a first conductive additive; forming a first mixture by drying the aqueous solution; forming a second mixture by mixing a second conductive additive and a binder; forming a third mixture by mixing the first mixture and the second mixture; and coating a current collector with the third mixture and reducing the oxidized derivative of the first conductive additive.

  2. Claim 2Depends on #1

    The method for manufacturing a storage battery electrode according to claim 1 , characterized by adding a reducing agent to the first mixture after forming the first mixture.

  3. Claim 3Independent Claim

    The method for manufacturing a storage battery electrode according t

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
JP H1125983 AActive material for lithium battery—162
JP 2002110162 APositive electrode active material and nonaqueous electrolytic battery—88
WO 2006/028476 A2Manganese oxide composite electrodes for lithium batteries—21
JP 2007200865 ANonaqueous electrolyte secondary battery—23
US 7,303,840 B2Manganese oxide composite electrodes for lithium batteries200791
JP 2008511960 Aリチウム電池用のマンガン酸化物複合電極—52
US 2009011335 A1Positive electrode active material, method of manufacturing the positive electrode active material, and non-aqueous electrolyte secondary battery—28
US 7,635,536 B2Manganese oxide composite electrodes for lithium batteries200927
US 7,790,308 B2Manganese oxide composite electrodes for lithium batteries201023
US 7,892,679 B2Non-aqueous electrolyte secondary battery20117
US 2011076564 A1Positive electrode active material, method of manufacturing the positive electrode active material, and non-aqueous electrolyte secondary battery using the positive electrode active material—35
US 2011200879 A1Non-aqueous electrolyte secondary battery and method of manufacturing the same—19
CN 102,163,739 ANon-aqueous electrolyte secondary battery and method of manufacturing the same—20
JP 2011170994 ANon-aqueous electrolyte secondary battery and method of manufacturing the same—25
WO 2011/111364 A1Method for producing composite oxide, positive electrode material for lithium ion secondary battery and lithium ion secondary battery—41
WO 2011/141486 A1Method for encapsulating metals and metal oxides with graphene and use of said materials—89
US 8,080,340 B2Manganese oxide composite electrodes for lithium batteries201126
US 2012088151 A1Positive-electrode active material and power storage device—39
WO 2012/046669 A1Positive-electrode active material and power storage device—8
US 2012088156 A1Method for manufacturing positive electrode active material for energy storage device and energy storage device—31
JP 2012099467 AMethod for manufacturing positive electrode active material for electrical storage device and electrical storage device—31
JP 2012099468 APositive electrode active material, and accumulator—37
WO 2012/088683 A1Porous graphene material and preparation method and uses as electrode material thereof—12
TW 201,230,477 APositive-electrode active material and power storage device—5
JP 2012169217 APositive electrode active material for lithium ion secondary battery, and method for manufacturing the same—118
WO 2012/124242 A1Cathode active material for non-aqueous electrolyte secondary battery, method for producing same, and non-aqueous electrolyte secondary battery using same—9
WO 2012/132387 A1Electrode material, method for producing same, electrode, secondary battery, and vehicle—39
US 2012308891 A1Method of manufacturing electrode—29
WO 2012/165358 A1Method of manufacturing electrode—23

Non-Patent Literature (5)

  • International Search Report (Application No. PCT/IB2015/059993) dated Apr. 19, 2016.
  • McCalla.E et al., “The spinel and cubic rocksalt solid-solutions in the Li—Mn—Ni oxide pseudo-ternary system”, Solid State Ionics, May 2, 2013, vol. 242, pp. 1-9, Elsevier.
  • Tan.H et al., “Oxidation state and chemical shift investigation in transition metal oxides by EELS”, Ultramicroscopy, May 1, 2012, vol. 116, pp. 24-33, Elsevier.
  • Wang.Z et al., “EELS analysis of cation valence states and oxygen vacancies in magnetic oxides”, MICRON, Oct. 1, 2000, vol. 31, No. 5, pp. 571-580, Elsevier.
  • Written Opinion (Application No. PCT/IB2017/053050) dated Jul. 4, 2017.