US 10,364,490 B2#26743263 Most CitedActiveUnited States (USPTO)Utility

Chromizing over cathodic arc coating

4Forward Citations (#26743263 Global)
0.6/yrCitation Velocity (#14106282 Global)
1.17Citation PageRank (#33623518 Global)
13Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a Cr-rich cathodic arc coating, an article in turbine blade coated with the chromizing over cathodic arc coating, and a method to produce the coating thereof. The Cr-rich cathodic arc coating in the present invention comprises a cathodic arc coating and a diffusion coating deposited atop the cathodic arc coating to enforce hot corrosion resistance. The hardware coated with the chromizing over cathodic arc coating in the present invention is reinforced with superior-hot corrosion resistance. The present invention further provides a novel method for producing the chromizing over cathodic arc coating by re-sequencing coating deposition order. The method in the present invention is efficient and cost-reducing by eliminating some operations, e.g., DHT and peening, between the cathodic arc coating and the diffusion coating. The hot corrosion resistance in the present invention results from the high Cr content in the surface of the coating.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 4.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A chromium-rich cathodic arc coating comprising: a MCrAlY cathodic arc coating on a substrate, wherein M is a metal alloy comprising nickel, cobalt, iron, or a combination thereof and the cathodic arc coating comprises 25 to 50% chromium by weight based on the weight of the MCrAlY; and a diffused chromide coating atop the MCrAlY cathodic arc coating, wherein the diffused chromide coating has a higher content of chromium than the MCrAlY cathodic arc coating, the combined thickness of the diffused chromide coating and the MCrAlY cathodic arc coating is 2.5 to 3 mil (0.0635 to 0.0762 mm), and the

  2. Claim 2Depends on #1

    The chromium-rich cathodic arc coating according to claim 1 , wherein the surface of the diffused chromide coating atop

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • European Search Report for European Application No. 14869840.0 dated Jun. 20, 2017, 11 pages.
  • Notification of Transmittal of the International Search Report of the International Searching Authority, or the Declaration; PCT/US2014066277; dated Mar. 18, 2015. 3 pages.
  • Notification of Transmittal of the Written Opinion of the International Searching Authority, or the Declaration; PCT/US2014/066277; dated Mar. 18, 2015. 9 pages.