Method for producing a foam glass with high open pore content
Abstract
A method for producing foam glass with high open pore content using recycled waste glass. The size of the pores of the foam glass is small and uniform, and such foam glass is suitable for building material with thermal insulating and sound proofing properties. The foam glass produced by this method is lightweight, durable and has high compression strength.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 25 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for producing foam glass comprising the steps of: combining glass particles with foaming agents, additives and a binding agent to form a mixture; compressing the mixture in a mold with a compression pressure between 2 MPa and 20 MPa for a period of time between 30 seconds and 15 minutes to form a compressed sample; de-molding the sample and curing the sample; heating the sample to a first elevated temperature and maintaining the sample at the first elevated temperature for a first period of time to decompose a part of the foaming agents; heating the sample from the first elevated temp
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (25)
Non-Patent Literature (2)
- International Preliminary Report on Patentability for International Application No. PCT/SG2012/000129,Report dated Oct. 14, 2014, dated Oct. 23, 2014, 5 Pgs.
- International Search Report and Written Opinion for International Application No. PCT/SG2012/000129, Search completed May 10, 2012, dated May 18, 2012, 7 Pgs.