Patents
US 10,329,638 B2#61658584 Most CitedActiveUnited States (USPTO)Utility

High strength galvanized steel sheet and production method therefor

1Forward Citations (#61658584 Global)
0.1/yrCitation Velocity (#40757705 Global)
0.74Citation PageRank (#61658584 Global)
14Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A high strength galvanized steel sheet that has a tensile strength (TS) of 780 MPa or higher and excellent bendability, fatigue resistance, and surface appearance quality and a method for producing the high strength galvanized steel sheet. The steel sheet includes, at a position ½ of a thickness of the steel sheet, 5% or more and 80% or less of a ferrite phase in terms of area fraction, 20% or more and 70% or less of a martensite phase in terms of area fraction, and 0% or more and 25% or less of a bainite phase in terms of area fraction.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A high strength galvanized steel sheet having a composition comprising, in terms of % by mass, C: 0.05% or more and 0.15% or less, Si: 0.01% or more and 1.00% or less, Mn: 2.2% or more and 3.5% or less, P: 0.001% or more and 0.050% or less, S: 0.010% or less, sol. Al: 0.005% or more and 0.100% or less, N: 0.0001% or more and 0.0060% or less, at least one element selected from the group consisting of Nb: 0.01% or more and 0.10% or less and Ti: 0.01% or more and 0.10% or less, and the balance being Fe and unavoidable impurities, wherein a microstructure at a position ½ of a thickness of the stee

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (14)

PatentTitleYearCitations
JP 2,587,724 B2めっき密着性の良好な高Si含有高張力溶融亜鉛めっき鋼板の製造方法19978
JP 2002088459 AGalvanized steel sheet excellent in balance of strength- ductility and adhesion of plating and its production method—30
US 6,558,815 B1Hot dip Galvanized steel plate excellent in balance of strength and ductility and in adhesiveness between steel and plating layer200337
JP 2004263271 AMethod for manufacturing high-tensile galvanized steel plate—45
JP 3,956,550 B2強度延性バランスに優れた高強度溶融亜鉛メッキ鋼板の製造方法200717
WO 2010/137317 A1High-strength steel sheet, hot-dipped steel sheet, and alloy hot-dipped steel sheet that have excellent fatigue, elongation, and collision characteristics, and manufacturing method for said steel sheets—54
JP 2011179030 ASuper-high strength cold-rolled steel sheet having excellent bending properties—44
US 2012031528 A1High-strength steel sheet, hot-dipped steel sheet, and alloy hot-dipped steel sheet that have excellent fatigue, elongation, and collision characteristics, and manufacturing method for said steel sheets—50
JP 4,924,730 B2加工性、溶接性および疲労特性に優れる高強度溶融亜鉛めっき鋼板およびその製造方法20126
KR 20130006507 AHigh-strength molten-zinc-plated steel sheet having excellent bendability and weldability, and process for production thereof—24
US 2013048151 A1Ultra high strength cold rolled steel sheet having excellent bendability—23
JP 5,255,361 B2曲げ加工性および疲労強度に優れた高強度鋼板20131
JP 5,374,193 B2曲げ加工性および疲労強度に優れた溶融亜鉛めっき鋼板または合金化溶融亜鉛めっき鋼板20132
JP 5,434,960 B2曲げ性および溶接性に優れる高強度溶融亜鉛めっき鋼板およびその製造方法20145

Non-Patent Literature (4)

  • Oct. 11, 2017 Office Action issued in Chinese Patent Application No. 201580041171.1.
  • Sep. 13, 2018 Notice of Allowance issued in Korean Patent Application No. 10-2017-7002129.
  • Sep. 15, 2015 International Search report issued in International Patent Application No. PCT/JP2015/002904.
  • Sep. 15, 2015 Written Opinion issued in International Patent Application No. PCT/JP2015/002904.