A bonding material of a silver paste includes: fine silver particles having an average primary particle diameter of 1 to 50 nanometers, each of the fine silver particles being coated with an organic compound having a carbon number of not greater than 8, such as hexanoic acid; silver particles having an average primary particle diameter of 0.5 to 4 micrometers, each of the silver particles being coated with an organic compound, such as oleic acid; a solvent containing 3 to 7% by weight of an alcohol and 0.3 to 1% by weight of a triol; a dispersant containing 0.5 to 2% by weight of an acid dispersant and 0.01 to 0.1% by weight of phosphate ester dispersant; and 0.01 to 0.1% by weight of a sintering aid, such as diglycolic acid, wherein the content of the fine silver particles is in the range of from 5% by weight to 30% by weight, and the content of the silver particles is in the range of from 60% by weight to 90% by weight, the content of the total of the fine silver particles and the silver particles being not less than 90% by weight.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 1.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A bonding material of a silver paste comprising: fine silver particles having an average primary particle diameter of 1 to 50 nanometers; silver particles having an average primary particle diameter of 0.5 to 4 micrometers; a solvent; an acid dispersant; and a phosphate ester dispersant, wherein the content of the fine silver particles is in the range of from 5% by weight to 30% by weight, and the content of the silver particles is in the range of from 60% by weight to 90% by weight, the content of the total of the fine silver particles and the silver particles being not less than 90% by weigh

  2. Claim 2Depends on #1

    A bonding agent as set forth in claim 1 , wherein the amount of said phosphate ester dispersant is 0.01 to 0.1% by weight with respect to said silver paste.

  3. Claim 3Independent Claim

    A boding agent as set forth in claim

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (16)

PatentTitleYearCitations
JP 2010153118 AMetallic particle paste and method for manufacturing conductive substrate—35
JP 2011080147 AJoining material and joining method using the same—72
JP 2011240406 ABonding material and bonding method using the same—43
WO 2011/155055 A1Low-temperature-sintering bonding material and bonding method using the bonding material—15
JP 4,870,223 B1ペースト状銀粒子組成物、金属製部材接合体の製造方法および金属製部材接合体20129
JP 2012052198 APaste-like silver particle composition, method for manufacturing metallic member joined body, and metallic member joined body—67
US 2012114972 A1Composite Nanometal Paste of Two-Metallic-Component Type, Bonding Method, and Electronic Part—5
WO 2012/070262 A1Binding material, binding body, and binding method—19
JP 2013004309 AMetal nanoparticle paste—8
US 2013081759 A1Low-temperature-sinterable bonding material, and bonding method using the bonding material—16
EP 2,581,156 A1Low-temperature-sinterable bonding material, and bonding method using the bonding material—7
WO 2013/108408 A1Bonding material and bonding method in which said bonding material is used—47
US 2013323529 A1Bonding material and bonding body, and bonding method—12
US 8,641,929 B2Low-temperature-sinterable bonding material, and bonding method using the bonding material20149
US 2015028085 A1Bonding material and bonding method in which said bonding material is used—20
US 9,533,380 B2Bonding material and bonding method in which said bonding material is used20172

Non-Patent Literature (3)

  • Che et al., "Nanoparticles-aided Silver Front Contact Paste for Crystalline Silicon Solar Cells", J. Material Science: Material Electron (2013), 24, pp. 524-528.
  • International Search Report for PCT/JP2014/066916 dated Sep. 11, 2014.
  • Soichi et al., "Low-Temperature and Low-Pressure Die Bonding Using Thin Ag-Flake and Ag-Particle Pastes for Power Devices", IEEE Transactions on Components, Packaging and Manufacturing Technology, vol. 3, No. 6, Jun. 2013, pp. 923-929.