Patents
US 10,294,151 B2#60995087 Most CitedActiveUnited States (USPTO)Utility

Glasses and glass ceramics including a metal oxide concentration gradient

1Forward Citations (#60995087 Global)
0.1/yrCitation Velocity (#40710115 Global)
0.75Citation PageRank (#60995087 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Embodiments of a glass-based article including a first surface and a second surface opposing the first surface defining a thickness (t) of about 3 millimeters or less (e.g., about 1 millimeter or less), and a stress profile, wherein all points of the stress profile between a thickness range from about 0·t up to 0.3·t and from greater than 0.7·t, comprise a tangent that is less than about −0.1 MPa/micrometers or greater than about 0.1 MPa/micrometers, are disclosed. In some embodiments, the glass-based article includes a non-zero metal oxide concentration that varies along at least a portion of the thickness (e.g., 0·t to about 0.3·t). In some embodiments, the concentration of metal oxide or alkali metal oxide decreases from the first surface to a point between the first surface and the second surface and increases from the point to the second surface. The concentration of the metal oxide may be about 0.05 mol % or greater or about 0.5 mol % or greater throughout the thickness. Methods for forming such glass-based articles are also disclosed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A glass substrate comprising: from about 60 mol. % to about 70 mol. % SiO 2 ; from about 0 mol. % to about 5 mol. % MgO; from about 1 mol. % to about 2 mol. % CaO; and from about 2 mol. % to about 10 mol. % Li 2 O, wherein: a ratio of Li 2 O to R 2 O is greater than 0.5 and less than or equal to 1, wherein R 2 O is the sum (mol. %) of Li 2 O, K 2 O, and Na 2 O in the glass substrate; and the glass substrate is substantially free of TiO 2 ; and the glass substrate is substantially free of ZrO 2 .

  2. Claim 2Depends on #1

    The glass substrate of claim 1 further comprising from about 5 mol. % to about 28 mol. % Al 2 O 3 .

  3. Claim 3Depends on #1

    The glass substrate of claim 1 , wherein Al 2 O 3 is present in an amount from about 5 mol. % to about 20 mol. %.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
GB 1,026,770 AGlass article and method of treatment—54
US 3,357,876 AMethod of strengthening a glass article by ion exchange1967176
US 3,380,818 AGlass composition and method and product1968128
US 3,404,015 ALow thermal expansion glasses196841
US 3,433,611 AStrengthening glass by multiple alkali ion exchange1969228
US 3,464,880 ASurface crystallized glass and method of producing196994
US 3,490,984 AArt of producing high-strength surface-crystallized,glass bodies197071
US 3,625,718 ANew thermally crystallizable glasses and low expansion transparent translucent and opaque ceramics made therefrom197175
US 3,639,198 AGlass articles having improved breakage characteristics197255
US 3,656,923 AMethod for strengthening photochromic glass articles197256
US 3,660,060 AProcess of making glass lasers of increased heat dissipation capability197246
US 3,798,013 ADouble ion exchange method for strengthening glass articles1974232
US 3,811,855 AMethod of treating a glass body to provide an ion-depleted region therein197465
US 3,879,183 ACorona discharge method of depleting mobile ions from a glass region197570
US 3,907,577 AMaking surface crystallized glass bodies and resulting product1975113
US 3,959,000 AHigh strength glass made by ion exchange197660
US 4,042,405 AHigh strength ophthalmic lens197793
US 4,053,679 AChemically strengthened opal glass1977123
US 4,055,703 AIon exchange strengthened glass containing P2 O51977110
US 4,130,437 APhotochromic glasses suitable for simultaneous heat treatment and shaping197854
US 4,148,661 APhotochromic sheet glass compositions and method197963
US 4,156,755 ALithium containing ion exchange strengthened glass1979204
US 4,190,451 APhotochromic glass1980105
US 4,240,836 AColored photochromic glasses and method198089
US 4,358,542 APhotochromic glass suitable for microsheet and simultaneous heat treatment and shaping198239
US 4,407,966 AVery fast fading photochromic glass198333
US 4,468,534 AMethod and device for cutting glass198480
US 4,471,024 AMethod of manufacturing a tempered glass dielectric material for use as an electrical insulator and insulator fabricated therefrom198438