An aluminum alloy fin material for heat exchanger use having a 35 to 50 μm thickness, a small springback at the time of corrugation, a suitable strength before brazing enabling easy fin formation, a high strength after brazing, and excellent erosion resistance, self corrosion resistance, and sacrificial anodic effect and a method of production of the same are provided. A fin material containing, by mass %, Si: 0.9 to 1.2%, Fe: 0.8 to 1.1%, Mn: 1.1 to 1.4%, and Zn: 0.9 to 1.1%, further limiting the impurity Mg to 0.05% or less, Cu to 0.03% or less, and ([Si]+[Fe]+2[Mn])/3 to 1.4% to 1.6%, and having a balance of unavoidable impurities and Al. A method of production prescribing hot rolling, cold rolling, intermediate annealing, and final cold rolling.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An aluminum alloy fin material for heat exchanger use containing, by mass %, Si: 0.9 to 1.2%, Fe: 0.8 to 1.1%, Mn: 1.1 to 1.4%, and Zn: 0.9 to 1.1%, further limiting the impurity Mg to 0.05% or less, Cu to 0.03% or less, and concentration of content of ([Si]+[Fe]+2[Mn])/3 to 1.4% to 1.6%, and having a balance of unavoidable impurities and Al, wherein a final sheet thickness is 35 to 50 μm, a tensile strength before brazing is 215 MPa or less, a solidus temperature is 620° C. or more, a tensile strength after brazing is 140 MPa or more, an electrical conductivity after brazing is 45% IACS or mo

  2. Claim 2Depends on #1

    An aluminum alloy fin material for heat exchanger use according to claim 1 , wherein an electrical conductivity after brazing is 45% IACS to 46.3% IACS or less.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (1)

  • International Search Report from PCT/JP2013/065468 dated Aug. 6, 2013.