A cold rolled and annealed martensitic steel sheet is provided. The steel sheet includes by weight percent, 0.30≤C≤0.5%, 0.2≤Mn≤1.5%, 0.5≤Si≤3.0%, 0.02≤Ti≤0.05%, 0.001≤N≤0.008%, 0.0010≤B≤0.0030%, 0.01≤Nb≤0.1%, 0.2≤Cr≤2.0%, P≤0.02%, S≤0.005%, Al≤1%, Mo≤1% and Ni≤0.5%. The remainder of the composition includes iron and unavoidable impurities resulting from melting. The microstructure is 100% martensitic and a prior austenite grain size is lower than 20 μm. The steel sheet has a delayed fracture resistance of at least 24 hours during an acid immersion U-bend test. A method, part, structural member and vehicle are also provided.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A martensitic steel sheet, directly obtained after cold rolling, annealing and cooling, comprising, by weight percent: 0.30≤C≤0.5%; 0.2≤Mn≤1.5%; 0.5≤Si≤3.0%; 0.02≤Ti≤0.05%; 0.001≤N≤0.008%; 0.0010≤B≤0.0030%; 0.01≤Nb≤0.1%; 0.2≤Cr≤2.0%; P≤0.02%; S≤0.005%; Al≤1%; Mo≤1%; and Ni≤0.5%; the remainder of the composition being iron and unavoidable impurities resulting from melting; a microstructure being 100% tempered martensitic with a prior austenite grain size lower than 20 μm; the steel sheet having a delayed fracture resistance of at least 24 hours during an acid immersion U-bend test.

  2. Claim 2Depends on #1

    The cold rolled and annealed martensitic steel sheet according to claim 1 wherein 0.01≤Nb≤0.05%.

  3. Claim 3Depends on #1

    The cold rolled and annealed martensitic steel sheet according to claim 1 wherein 0.2≤Cr≤1.0%.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (3 of 3 total)

References Cited — Backward Prior Art (17)

PatentTitleYearCitations
US 4,201,574 ALow carbon Ni-Cr austenitic steel having an improved resistance to stress corrosion cracking19809
JP H0841535 AProduction of high hardness wear resistant steel excellent in low temperature toughness—70
RU 2,203,965 C2Cold rolled strip manufacture method200310
RU 2,235,136 C1Method for producing of sheet steel and saws, steel and products obtained therefrom200416
JP 2005097725 ASteel sheet for hot press having hydrogen embrittlement resistance, automobile member and its production method—103
WO 2007/129676 A1Hot-pressed steel sheet member and process for production thereof—49
JP 2010248565 AUltrahigh-strength cold-rolled steel sheet superior in formability for extension flange, and method for manufacturing the same—42
US 2011253271 A1High-strength steel plate and producing method therefor—16
JP 2012180594 AHot-press molded steel sheet member, steel sheet for hot-pressed steel sheet member, and method for producing them—71
CN 102,770,568 AUltra-high strength cold rolled steel sheet having excellent bendability—20
WO 2012/153009 A1Method for the production of very-high-strength martensitic steel and sheet thus obtained—5
CA 2,850,044 A1Hot-dip galvanized steel sheet and manufacturing method thereof—6
US 2013095347 A1Hot-stamped steel, method of producing of steel sheet for hot stamping, and method of producing hot-stamped steel—46
JP 2013104081 AHigh strength steel plate of excellent delayed fracture resistance, and method of producing the same—39
WO 2013/082188 A1Martensitic steels with 1700-2200 mpa tensile strength—12
US 2014144559 A1Method for production of martensitic steel having a very high yield point and sheet or part thus obtained—3
US 8,951,367 B2Ultra high strength cold rolled steel sheet having excellent bendability20154

Non-Patent Literature (3)

  • Machine English translation of JP 2010-174282, Kobayashi Satoo et al., Aug. 12, 2010.
  • Machine-English translation of JP 2010-150612, Takebayashi Shigeto et al., Jul. 8, 2010.
  • Tetsuo Shiraga, Nobuyuki Ishikawa, Moriyuki Ishiguro, Eiji Yamashita, Shigeru Mizoguchi, Effect of Ni, Cu and Si on Delayed Fracture Properties of High Strength Steels with Tensile Strength of 1450N/mm2, CAMP-ISIJ, vol. 7 (1994)-1646-1649.