Patents
US 10,170,764 B2#62833925 Most CitedActiveUnited States (USPTO)Utility

Method for manufacturing ultra small particle, positive electrode active material of second battery using the method for manufacturing ultra small particle and method for manufacturing the same, and secondary battery using the positive electrode active material and method for manufacturing the same

0Forward Citations (#62833925 Global)
0.0/yrCitation Velocity (#62833925 Global)
0.56Citation PageRank (#62833925 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An object is to form a positive electrode active material having small and highly uniform particles by a simple process. A template is formed by forming holes in the template by a nanoimprinting method, and the template is filled with a gel-like LiFePO4 material, whereby small-sized LiFePO4 particles are formed and are used as the positive electrode active material of a secondary battery. The particle size can be reduced to less than 50 nm. Further, when the LiFePO4 particles are sintered, the template may be burned down. By making the particle size of the positive electrode active material smaller than the conventional one, a positive electrode that lithium is injected into and extracted from easily can be manufactured.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a particle comprising: forming a material film over a substrate; forming a first protrusion in the material film; manufacturing a template including a second hole using the material film including the first protrusion; and filling the second hole in the template with a gel comprising a first material and a second material, whereby a particle is formed in the second hole; separating the particle from the template by heating, wherein a diameter of the particle is greater than or equal to 10 nm and less than or equal to 50 nm.

  2. Claim 2Depends on #1

    The method for manufacturing the particle according to claim 1 , wherein the first protrusion in the material film is formed by a nanoimprinting method.

  3. Claim 3Depends on #1

    The method for manufacturing the particle according to claim 1 , wherein the second hole in

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
JP 2003200051 ACatalyst for oxygen oxidation-reduction device and electrode using the same—32
JP 2005095733 AManufacturing method for particulate—15
JP 2006108649 AMetallic mold for nano-imprint, forming method of nano-pattern, and resin molding—12
JP 2007022894 AMethod for producing lithium-iron multiple oxide—31
WO 2007/024323 A2Nanoparticle fabrication methods, systems, and materials—81
WO 2007/030698 A2Materials and methods for fabricating isolated micro-and nano-structures having chemical functionality—21
WO 2005/101466 A3Methods for fabricating isolated micro- and nano- structures using soft or imprint lithography—2
JP 2007526820 Aソフトリソグラフィー又はインプリントリソグラフィーを用いる分離微小構造及び分離ナノ構造の作製方法—31
WO 2007/113624 A1Synthesis of nanoparticles of lithium metal phosphate positive material for lithium secondary battery—48
US 2007264481 A1Isolated and fixed micro and nano structures and methods thereof—130
WO 2008/011051 A1Nanoparticle fabrication methods, systems, and materials—4
WO 2008/018936 A2High fidelity nano-structures and arrays for photovoltaics and methods of making the same—21
WO 2007/000251 A8Crystalline nanometric lifepo4—1
WO 2008/063204 A2Taggants and methods and systems for fabricating—8
WO 2008/089110 A1Three-dimensional batteries and methods of manufacturing the same—28
US 2008181958 A1Nanoparticle fabrication methods, systems, and materials—20
WO 2008/093551 A1Compound having olivine structure, method for producing the same, positive electrode active material using compound having olivine structure, and nonaqueous electrolyte battery—12
WO 2008/106503 A2Discrete size and shape specific pharmaceutical organic nanoparticles—16
US 2008241690 A1Crystalline Nanometric LiFePO4—38
WO 2007/094829 A3Isolated and fixed micro and nano structures and methods thereof—1
WO 2008/013952 A3Nanoparticle fabrication methods, systems, and materials for fabricating artificial red blood cells—1
JP 2008546629 A結晶状のナノメーターLiFePO4—7
CN 101,415,640 ASynthesis of lithium metal phosphatic nanometer particle for lithium secondary battery anode material—23
US 2009186275 A1Synthesis of nanoparticles of lithium metal phosphate positive material for lithium secondary battery—46
WO 2009/105773 A2Lithium-ion battery—29
US 2009220789 A1Taggants and methods and systems for fabricating same—51
JP 2009532323 Aリチウム二次電池用のリチウム金属リン酸塩正極物質のナノ粒子の合成—41
JP 2010508234 A炭素処理複合酸化物及びその製造方法—22
US 7,696,100 B2Method for manufacturing semiconductor device20107
WO 2010/046629 A1Synthesis of metal compounds—17

Non-Patent Literature (4)

  • Chou et al., "Nanoimprint lithography", Journal of Vacuum Science & Technology B, Nov. 1, 1996, vol. 14, No. 6, pp. 4129-4133.
  • Chou, et al., " Sub-10 nm imprint lithography and applications", Journal of Vacuum Science & Technology B, Nov. 1, 1997, vol. 15, No. 6, pp. 2897-2904.
  • Croce, et al., "A Novel Concept for the Synthesis of an Improved LiFePO4 Lithium Battery Cathode", Electrochemical and Solid-State Letters, Jan. 24, 2002, vol. 5, No. 3, pp. A47-A50, ECS(The Electrochemical Society).
  • Kang, et al., "Battery materials for ultrafast charging and discharging", Nature, Mar. 12, 2009, vol. 458, No. 12, pp. 190-193.