US 10,165,713 B2#40859964 Most CitedActiveUnited States (USPTO)Utility

Advanced non-toxic radiation shielding materials from tailored brine sludge and a process for the preparation thereof

2Forward Citations (#40859964 Global)
0.2/yrCitation Velocity (#29049607 Global)
0.99Citation PageRank (#42203921 Global)
6Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Conventional shielding materials are based on single material either toxic lead or barium based compounds and any matrix made therefrom contains only single phased barium based compounds, thereby posing limited radiation shielding capacity. Since brine sludge, an industrial toxic waste product, generated in chloralkali industry contains multiple compounds; there is a need to provide a process which enables the preparation of multi-phase based radiation shielding materials. In view of the above, the present invention provides advanced non-toxic radiation shielding materials utilizing tailored brine sludge and a process that enables conversion of toxic elements like chromium, zinc, copper and vanadium present in brine sludge into non-toxic shielding phases, thereby enabling to convert a toxic waste material into highly value added advanced radiation shielding materials possessing homogeneous radiation shielding matrix.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 2.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An advanced non-toxic radiation shielding material comprising: [a] 200 g to 600 g of brine sludge; and [b] 20 g to 60 g of sodium hexametaphosphate.

  2. Claim 2Independent Claim

    A process for an advanced non-toxic radiation shielding material comprising the steps of: [a] drying 200 g to 600 g of brine sludge in an air oven at a temperature of 100 to 110° C. for a period of 1 to 2 hours; [b] heating the dried brine sludge as obtained in step [a] in a furnace at a temperature ranging from 800 to 1300° C. for a period of 1 to 2 hours; [c] mechano-chemical processing of the heat treated brine sludge obtained in step [b] by grinding with 20 to 60 g of sodium hexametaphosphate in a ball mill or planetary mill for a period of 1 to 6 hours to obtain tailored brine sludge powd