Abstract

Disclosed is a method of forming back end of the line (BEOL) metal levels with improved dielectric capping layer to metal wire adhesion. The method includes process step(s) designed to address dielectric capping layer to metal wire adhesion, when the metal wire(s) in a given metal level are relatively thick. These process step(s) can include, for example: (1) selective adjustment of the deposition tool used to deposit the dielectric capping layer onto metal wires based on the pattern density of the metal wires in order to ensure that those metal wires actually achieve a temperature between 360° C.-400° C.; and/or (2) deposition of a relatively thin dielectric layer on the dielectric capping layer prior to formation of the next metal level in order to reduce the tensile stress of the metal wire(s) below without causing delamination. Also disclosed is an IC chip formed using the above-described method.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method comprising: forming a metal level above a substrate, the forming of the metal level comprising: forming a first dielectric layer above the substrate, the first dielectric layer having a first thickness; forming trenches in the first dielectric layer; filling the trenches with copper to form copper wires; forming a second dielectric layer immediately adjacent to the first dielectric layer and the copper wires, the second dielectric layer having a second thickness and comprising a silicon nitride layer, and the forming of the second dielectric layer being performed using a plasma-enhanc

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (23)

PatentTitleYearCitations
US 5,447,887 AMethod for capping copper in semiconductor devices1995298
US 6,174,793 B1Method for enhancing adhesion between copper and silicon nitride200125
US 6,245,663 B1IC interconnect structures and methods for making same200195
US 6,251,775 B1Self-aligned copper silicide formation for improved adhesion/electromigration200134
US 6,303,505 B1Copper interconnect with improved electromigration resistance200176
EP 1,168,427 A1Method of plasma depositing silicon nitride—20
US 6,339,025 B1Method of fabricating a copper capping layer200233
US 6,429,128 B1Method of forming nitride capped Cu lines with reduced electromigration along the Cu/nitride interface200262
US 2003132510 A1Advanced BEOL interconnect structures with low-k PE CVD cap layer and method thereof—19
US 6,660,634 B1Method of forming reliable capped copper interconnects200366
US 6,743,310 B1Method of forming nitride capped Cu lines with improved adhesion and reduced electromigration along the Cu/nitride interface200416
US 6,803,325 B2Apparatus for improving barrier layer adhesion to HDP-FSG thin films20049
US 6,821,890 B2Method for improving adhesion to copper200435
US 6,977,218 B2Method for fabricating copper interconnects200522
US 7,157,798 B1Selective refractory metal and nitride capping200715
US 7,176,571 B2Nitride barrier layer to prevent metal (Cu) leakage issue in a dual damascene structure200719
US 7,202,162 B2Atomic layer deposition tantalum nitride layer to improve adhesion between a copper structure and overlying materials200715
US 7,534,732 B1Semiconductor devices with copper interconnects and composite silicon nitride capping layers200910
US 2010052172 A1Method of fabricating copper damascene and dual damascene interconnect wiring—5
US 7,678,699 B2Method of forming an insulating capping layer for a copper metallization layer by using a silane reaction20106
US 2012032333 A1Semiconductor device and method of manufacturing the same—11
US 8,450,191 B2Polysilicon films by HDP-CVD20136
CN 103,839,882 ASandwiched diffusion barrier and metal liner for an interconnect structure—7

Non-Patent Literature (5)

  • Chinese Application No. 201610258553.6, Office Action dated Aug. 28, 2018, pp. 1-7.
  • Chinese Application No. 201610258553.6, Search Report dated Aug. 20, 2018, pp. 1-2.
  • Hymes et al., "Passivation of Copper by Silicide Formation in Dilute Silane", Journal of Applied Physics, 71, 4623, 1992, pp. 1-4, http://dx.doi.org/10.1063/1.350765.
  • Notice of Allowance, U.S. Appl. No. 14/749,817, dated Mar. 27, 2017, pp. 1-8.
  • Office Action Communication, U.S. Appl. No. 14/749,817, dated Apr. 15, 2016, pp. 1-5.