Patents
US 10,160,063 B2#85178108 Most CitedActiveUnited States (USPTO)Utility

Braze materials and earth-boring tools comprising braze materials

0Forward Citations (#85178108 Global)
0.0/yrCitation Velocity (#85178108 Global)
0.56Citation PageRank (#85178108 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method includes disposing a braze material adjacent a first body and a second body; heating the braze material and forming a transient liquid phase; and transforming the transient liquid phase to a solid phase and forming a bond between the first body and the second body. The braze material includes copper, silver, zinc, magnesium, and at least one material selected from the group consisting of nickel, tin, cobalt, iron, phosphorous, indium, lead, antimony, cadmium, and bismuth.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A braze material comprising: copper; from about 50% to about 70% silver by weight; from about 25% to about 35% zinc by weight; magnesium; and at least one material selected from the group consisting of nickel, tin, cobalt, iron, phosphorous, indium, lead, antimony, cadmium, and bismuth.

  2. Claim 2Depends on #1

    The braze material of claim 1 , wherein the braze material comprises metallic particles having an average particle size in a range from about 1 μm to about 15 μm.

  3. Claim 3Depends on #1

    The braze material of claim 1 , further comprising an organic binder.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 2,781,577 AMethod of making corrosion resistant soldered joints195721
US 3,560,172 AIron-silicon magnetostrictive laminated material and elements197118
DE 2,112,418 A1Weichlot—2
US 3,684,496 ASolder having improved strength at high temperatures19727
US 3,783,037 ATreatment of alloys197443
US 3,999,962 ACopper-chromium carbide-metal bond for abrasive tools197632
US 4,008,844 AMethod of repairing surface defects using metallic filler material1977132
CH 588,910 A5Cutting tools with bits of cobalt base alloy - attached to tool shank by induction brazing, and giving reduced tool cost—7
US 4,049,475 ASECo5 -Permanent magnet joined to at least one iron mass and method of fabricating such a permanent magnet197713
US 4,073,639 AMetallic filler material197868
GB 2,027,617 AFlux coated brazing materials—10
US 4,350,215 ADrill bit and method of manufacture1982117
US 4,451,541 ASoldering composition and method of use198436
US 4,661,180 AMethod of making diamond tool198724
US 4,766,040 ATemperature resistant abrasive polycrystalline diamond bodies1988195
US 4,919,220 ACutting structures for steel bodied rotary drill bits1990107
US 5,056,382 AMatrix diamond drag bit with PCD cylindrical cutters199167
EP 0,541,071 A1Polycrystalline diamond cutting tool and method of manufacturing the same—36
JP H05140769 APolycrystalline diamond tool material and method for joining the same to base material of tool—14
US 5,221,039 ALiquid phase diffusion bonding using high diffusivity element as insert material199322
US 5,234,152 ATransient liquid phase ceramic bonding199371
JP H08238564 AMethod for forming metal joint—5
US 5,806,751 AMethod of repairing metallic alloy articles, such as gas turbine engine components199898
US 5,872,051 AProcess for transferring material to semiconductor chip conductive pads using a transfer substrate1999173
US 6,027,957 AControlled solder interdiffusion for high power semiconductor laser diode die bonding200046
US 6,044,920 ARotatable cutting bit assembly with cutting inserts200044
US 6,199,747 B1High temperature refractory joining paste200131
DE 10,060,136 A1Circular knife esp. for food slicing machines has cutting plates of hard metal soldered into pockets in main knife body—5
US 2002092895 A1Formation of a solder joint having a transient liquid phase by annealing and quenching—29

Non-Patent Literature (4)

  • Cook, III, Grant O., Joining Polycrystalline Cubic Boron Nitride and Tungsten Carbide by Partial Transient Liquid Phase, Theses and Dissertations, Paper 2366, (2010), 261 pages (5 part document).
  • Kang et al. “Istothermal Solidification of Cu/Sn Diffusion Couples to Form Thin-Solder Joints”, 2002.
  • MacDonald et al., Transient Liquid Phase Bonding, Annu. Rev. Mater. Sci., vol. 22, (1992), pp. 23-46.
  • Quintero, Pedro, O., Development of a Shifting Melting Point Ag—In Paste Via Transient Liquid Phase Sintering for High Temperature Environments, Dissertation, University of Maryland, (2008), 245 pages.