Golf ball incorporating at least one layer of neutralized acid polymer composition containing low molecular weight acid wax(es) as sole acid polymer component and method of making

2Forward Citations (#38891018 Global)
0.2/yrCitation Velocity (#28902052 Global)
1.04Citation PageRank (#39310645 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A golf ball comprising at least one layer comprised of a neutralized acid polymer composition consisting of a mixture of: (a) at least one low molecular weight acid-containing wax; (b) at least one non-acid-polymer; and (c) at least one organic acid or salt thereof. Each low molecular weight acid-containing wax may have a molecular weight of from about 500 to about 7000, and in some embodiments, the molecular weight may be considered low up to 30,000. Interactions between components (a), (b) and (c) as disclosed herein advantageously produce a layer of ionomeric material having desirable physical properties, such as heat stability, and processability (excellent melt flow) without the need for blending high and low molecular weight acid-containing polymer(s).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A golf ball comprising at least one layer consisting of a neutralized acid polymer composition consisting of a mixture of: (a) at least one low molecular weight acid-containing wax; (b) at least one non-acid-polymer; and (c) at least one organic acid or salt thereof; wherein each low molecular weight acid-containing wax has a molecular weight of from about 500 to about 30,000; wherein the mixture contains at least 70 percent of neutralized acid groups; and wherein the mixture has a melt flow index of at least 0.5 g/10 min.

  2. Claim 2Depends on #1

    The golf ball of claim 1 , wherein component (a) is included in an amount of 5 to 95 parts of each 100 parts of components (a) and (b) combined.

  3. Claim 3Depends on #2

    The golf ball of claim 2 , wherein component (b) is included in an amount of from about 5 to 95 parts of each 100 parts of components

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,625,964 AGolf ball1986347
US 5,048,838 AThree-piece solid golf ball1991291
US 5,104,126 AGolf ball1992419
US 5,306,760 AImproved golf ball cover compositions containing high levels of fatty acid salts1994407
US 5,312,857 AGolf ball cover compositions containing high levels of metal stearates1994348
US 5,334,673 APolyurethane golf ball1994923
US 5,480,155 AGolf ball1996118
US 5,482,285 AThree-piece solid golf ball1996417
US 5,484,870 APolyurea composition suitable for a golf ball cover1996724
US 2001014446 A1Assay methods for nucleic acid in a sample—22
US 6,277,034 B1Three piece golf ball with a spherical metal center2001196
US 6,315,683 B1Hollow solid golf ball200140
US 6,416,425 B1Solid golf ball200283
US 6,419,595 B1Solid golf ball2002106
US 6,461,251 B1Solid golf ball200286
US 6,494,795 B2Golf ball and a method for controlling the spin rate of same2002192
US 6,500,076 B1Wound golf balls with high specific gravity centers2002137
US 6,506,851 B2Golf ball comprising saturated polyurethanes and methods of making same2003219
US 2003013549 A1Golf balls comprising highly-neutralized acid polymers—72
US 6,527,652 B1Solid golf ball200386
US 6,596,815 B1Ionomer/high density polyethylene blends with improved flow200311
US 6,688,991 B2Golf ball with foam core and filled cover2004154
US 6,692,380 B2Golf ball with high density center2004123
US 2004106736 A1Golf ball—20
US 6,756,436 B2Golf balls comprising highly-neutralized acid polymers2004188
US 6,756,443 B2Ionomer/polyamide blends with improved flow and impact properties200444
US 6,762,246 B2Bi-modal ionomers200444
US 6,815,480 B2Highly-resilient thermoplastic elastomer compositions2004104

Non-Patent Literature (4)

  • Dalton, Jeff, Compression by Any Other Name, Science and Golf IV, Proceedings of the World Scientific Congress of Golf ( Eric Thain ed., Routledge, 2002)("J. Dalton").
  • Dupont, Hardness Conversion, uploaded Oct. 4, 2016, Dupont, 1 page.
  • Honeywell A-C580 product brochure; Jan. 2008.
  • Rick White, Shore Durometer Conversion Chart, uploaded Oct. 4, 2016, Thermal Tech Equipment, 1 page.