Cobalt-free, galling and wear resistant austenitic stainless steel hard-facing alloy
Abstract
A strain-hardenable stainless steel alloy includes hard secondary phases dispersed in an austenitic primary phase, the alloy including 0.3-0.6% nitrogen by weight.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 1.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of making a hard-faced metallic component, comprising: bonding a layer of a stainless steel alloy in powder form to a surface of a metallic component, such that the layer defines an outer surface, wherein the stainless steel alloy is void of cobalt and comprises hard secondary phases dispersed in an austenitic primary phase, the alloy consisting essentially of, by weight: 21.0 to 27.0% chromium; 3.0 to 7.0% manganese; 2.0 to 6.0% nickel; 1.5 to 4.0% silicon; 1.0 to 5.0% molybdenum; 0.9 to 1.3% carbon; 0.44-0.55% nitrogen; the balance iron and impurities; hot isostatic pressing (“HIP”)
- Claim 2Independent Claim
The me
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| CN 109,609,731 A | A kind of high chromium mill forging same temperature hardening heat treatment process | — | 2 |
References Cited — Backward Prior Art (11)
Non-Patent Literature (1)
- Machine-English translation of Chinese patent 101338385A, "Nitrogen-containing/high nitrogen stainless steel products and Method fo preparing same," Chunjiang Kuang et al. Jan. 7, 2009.