Patents
US 10,086,246 B2#124030818 Most CitedActiveUnited States (USPTO)Utility

Golf club fabricated from bulk metallic glasses with high toughness and high stiffness

0Forward Citations (#124030818 Global)
0.0/yrCitation Velocity (#124030818 Global)
0.56Citation PageRank (#124030818 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Golf clubs formed from bulk-solidifying amorphous metals (i.e., metallic glasses) having high elastic modulus and fracture toughness, and to methods of forming the same are provided. Among other components, the golf club materials disclosed enable fabrication of flexural membranes or shells used in golf club heads (drivers, fairways, hybrids, irons, wedges and putters) exhibiting enhanced flexural or bending compliance together with the ability to deform plastically and avoid brittle fracture or catastrophic failure when overloaded under bending loads. Further, the high strength of the material and its density, comparable to that of steel, enables the redistribution of mass in the golf club while maintaining a desired overall target mass.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A golf club striking face, wherein at least a portion of the golf club striking face is formed from a metallic glass having an elastic strain limit of at least 1.4%, a Young's modulus greater than 120 GPa, and a notch toughness, defined as the stress intensity factor at crack initiation when measured on a 3 mm diameter rod containing a notch with length ranging from 1 to 2 mm and root radius ranging from 0.1 to 0.15 mm, of at least 50 MPa-m 1/2 , and wherein the metallic glass forming the golf club striking face has a critical plate thickness of at least 1 mm, whereby a ratio of the stored

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,856,513 ANovel amorphous metals and amorphous metal articles1974332
US 4,252,262 AMethod for manufacturing a golf club1981161
US 4,298,382 AMethod for producing large metallic glass bodies198127
US 4,455,177 AMethod and apparatus for chemical heat treatment of steel parts utilizing a continuous electric furnace198437
US 4,699,383 AClub-head198740
US 4,708,347 AClub-head198763
US 4,754,975 AIron club head198858
US 4,802,844 AHigh capacity, retractable furnace hearth19897
US 4,857,414 AAmorphous metal-metal composite article and a method for producing the same198911
US 4,928,965 AGolf club and method of designing same1990160
US 4,965,139 ACorrosion resistant metallic glass coatings199024
US 4,964,927 AAluminum-based metallic glass alloys199070
US 5,024,437 AGolf club head1991208
US 5,032,196 AAmorphous alloys having superior processability1991120
US 5,074,935 AAmorphous alloys superior in mechanical strength, corrosion resistance and formability199166
US 5,094,383 AGolf club head and method of forming same1992246
US 5,188,152 ATubular structures for fishing rods or the like199322
US 5,208,090 AMetal single fiber-reinforced prepreg199327
JP H0533071 U多芯線電線絶縁チエツカー—3
US 5,213,148 AProduction process of solidified amorphous alloy material199368
US 5,226,652 AGolf club with improved impact property199339
US 5,255,918 AGolf club head and method of forming same1993181
US 5,261,663 AGolf club head and method of forming same1993175
US 5,261,664 AGolf club head and method of forming same1993259
US 5,266,027 ARoller-hearth continuous furnace199323
US 5,288,344 ABerylllium bearing amorphous metallic alloys formed by low cooling rates1994481
US 5,344,140 AGolf club head and method of forming same1994265
US 5,368,659 AMethod of forming berryllium bearing metallic glass1994316
US 5,417,419 AGolf club with recessed, non-metallic outer face plate1995141
US 5,421,724 ARolls for high temperature roller hearth furnaces199520

Non-Patent Literature (5)

  • Bruck et al., “Quasi-Static Constitutive Behavior of Zr41.25Ti1.75Ni10Be12.5 Bulk Amorphous Alloys”, Scripta Metallurgica et Materialia, 1994, vol. 30, pp. 429-434.
  • Inoue et al., “Mg-Cu-Y Bulk Amorphous Alloys with High Tensile Strength Produced by a High-Pressure Die Casting Method”, Materials Transaction, JIM, 1992, vol. 33, No. 10, pp. 937-945.
  • Inoue et al., “Production of Amorphous Cylinder and Sheet of La55Al25Ni20 Alloy by a metallic Mold Casting Method”, Materials Transactions, JIM, 1990, vol. 31, No. 5, pp. 425-428.
  • International Preliminary Report on Patentability for International Application PCT/US2014/013625, issued Aug. 4, 2015, dated Aug. 13, 2015, 5 pgs.
  • International Search Report and Written Opinion for International Application No. PCT/US2014/013625, Completed May 5, 2014, dated May 15, 2014, 5 pgs.