Abstract

An improved anti-reflection glass with higher transmittance (ΔTqe %) results from a coating of or including tin oxide (e.g., SnO2) nanoparticles (e.g., 10-20 nm in size) applied to a surface of solar float or matte/matte glass. The tin oxide based coating layer shows improved chemical stability and durability and can be prepared using a sol-gel process and applied by spin coating. Matte/matte anti-reflection glass samples may have two coating layers (e.g., SnO2 nanoparticles on the rough side and SiO2 nanoparticles on the smooth side) and exhibit an improved transmittance (e.g., visible transmittance) of at least 2.0%, e.g., about 3.5%. As high as a 30% increase of ΔTqe % has been observed when anti-reflection matte/matte glass coated with SnO2 is exposed in a salt fog chamber for 5 days. The increase in transmittance may be due to the different pore structure of the SnO2 coating layer, while the increase of Tqe % in a salt fog chamber may be due to the crystalline SnO2 formation.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a coated article with an anti-reflection coating, the method comprising: forming a coating consisting essentially of silica particles and a binder directly on a first surface of a glass substrate; and forming a coating comprising tin oxide directly on a second surface of the glass substrate, wherein the glass substrate is disposed between the silica coating and the tin oxide coating.

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein forming the coating comprising tin oxide comprises depositing at least a portion of a colloidal solution comprising the tin oxide on a glass substrate; and curing the coating comprising tin oxide at least by heating said glass substrate and the coating comprising tin oxide.

  3. Claim 3Depends on #2

    The method according to claim 2 , wherein said colloidal solution contain

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

PatentTitleYearCitations
US 2019154882 A1Antireflection film—2

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,607,322 ALight transmitting glass fibers, core and cladding glass compositions197125
US 4,510,344 AThin film solar cell substrate198586
JP S62289801 AAntistatic antireflective molding—8
US 4,806,436 ASubstrate for amorphous silicon solar cells1989128
US 4,945,282 AImage display panel having antistatic film with transparent and electroconductive properties and process for processing same199095
US 5,091,764 ASemiconductor device having a transparent electrode and amorphous semiconductor layers199239
US 5,189,337 AUltrafine particles for use in a cathode ray tube or an image display face plate199360
JP H07122764 AManufacture of solar battery substrate—48
WO 9,513,993 A1Lead-free crystal glass with the refractive index higher than 1,52—68
EP 0,702,390 A1Antireflection type cathode-ray tube and method of manufacturing the same—2
WO 9,715,935 A1Electrically conductive transparent film and coating composition for forming such film—20
US 5,742,118 AUltrafine particle film, process for producing the same, transparent plate and image display plate199881
EP 0,871,046 A1Anti-fogging coating and optical part using the same—38
WO 9,937,720 A1Antisoiling coatings for antireflective surfaces and methods of preparation—65
US 5,977,477 APhotovoltaic device1999101
US 5,997,943 ACompound for a non-wettable coating, process for treatment of glass with the aid of the compound and products obtained199945
WO 0,010,934 A1Process for producing durable antireflective surfaces and antireflective articles—73
US 6,190,776 B1Heat treatable coated glass200129
US 6,312,808 B1Hydrophobic coating with DLC & FAS on substrate2001102
EP 1,167,313 A1Low-reflection glass article—53
US 2002014090 A1Low-reflection glass article—34
US 6,350,397 B1Optical member with layer having a coating geometry and composition that enhance cleaning properties200245
US 2002192380 A1Compositions comprising fluorinated silanes and compressed fluid CO2—47
US 6,506,622 B1Method of manufacturing a photovoltaic device2003101
US 6,610,622 B1Clear glass composition200396
US 2003180544 A1Anti-reflective hydrophobic coatings and methods—23
US 2004028819 A1Composition and method for a coating providing anti-reflective and anti-static properties—3
US 6,706,398 B1Organosilicon compounds and blends for treating silica200420
US 2004156984 A1UV-reflective interference layer system—23

Non-Patent Literature (5)

  • "The Electrical and Optical Properties of Thin Layers of Nano-Sized Antimony Doped Tinoxide Particles"; Van Bommel et al., Journal of Materials Science 34 (1999), pp. 4803-4809.
  • EP Search Report dated Jun. 3, 2014 for EP 13196930.5.
  • EP Search Report dated Jun. 3, 2014 for EP 13196999.0.
  • U.S. Appl. No. 13/360,898, filed Jan. 30, 3012; Lewis et al.
  • U.S. Appl. No. 13/361,754, filed Jan. 30, 2012; Lewis et al.